Final Magnetic Moment3.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.492 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.258 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 173.0 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 230.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 230.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 288.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 268.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 67.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 230.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 57.7 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 259.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 268.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 134.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 230.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 67.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 67.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 230.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 57.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 288.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 230.7 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 268.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 67.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 288.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 268.1 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 230.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 173.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 173.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 288.4 |
BN (mp-984) | <1 0 1> | <1 0 0> | 268.1 |
BN (mp-984) | <1 1 0> | <1 0 1> | 265.3 |
Al (mp-134) | <1 0 0> | <1 0 1> | 265.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 288.4 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 134.0 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 230.7 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 201.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 57.7 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 230.7 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 230.7 |
C (mp-66) | <1 1 0> | <0 0 1> | 288.4 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 134.0 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 230.7 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 67.0 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 265.3 |
Mg (mp-153) | <1 1 0> | <1 1 1> | 259.2 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 268.1 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 173.0 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 268.1 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 201.1 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 134.0 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 230.7 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 67.0 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 230.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.31 | 0.00 | -0.00 |
0.00 | 2.31 | 0.00 |
-0.00 | 0.00 | 2.40 |
Dielectric Tensor εij (total) |
||
---|---|---|
5.07 | 0.00 | -0.00 |
0.00 | 5.07 | 0.00 |
-0.00 | 0.00 | 5.66 |
Polycrystalline dielectric constant
εpoly∞
2.34
|
Polycrystalline dielectric constant
εpoly
5.26
|
Refractive Index n1.53 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TlSbF6 (mp-8348) | 0.1488 | 0.000 | 3 |
RbRuF6 (mp-8014) | 0.1638 | 0.000 | 3 |
KAsF6 (mp-7569) | 0.1558 | 0.000 | 3 |
KCrF6 (mp-606564) | 0.2071 | 0.000 | 3 |
KCrF6 (mp-561183) | 0.2077 | 0.000 | 3 |
Cs4TlSbCl12 (mp-650007) | 0.6659 | 0.000 | 4 |
Cs2TlSiH6 (mp-989560) | 0.6594 | 0.015 | 4 |
Cs2SeClF6 (mp-989544) | 0.7110 | 0.000 | 4 |
Cs4BiSbCl12 (mp-23583) | 0.7016 | 0.000 | 4 |
LiMgH6Ir (mp-866640) | 0.6244 | 0.000 | 4 |
Rb19O3 (mp-779582) | 0.5652 | 0.043 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Ru_pv F |
Final Energy/Atom-4.8288 eV |
Corrected Energy-41.4022 eV
Uncorrected energy = -38.6302 eV
Composition-based energy adjustment (-0.462 eV/atom x 6.0 atoms) = -2.7720 eV
Corrected energy = -41.4022 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)