material

AlF3

ID:

mp-8039

DOI:

10.17188/1307908


Tags: Aluminium fluoride - alpha Aluminium trifluoride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.891 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.001 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.89 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
AlF3
Band Gap
7.693 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 130021 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.000 149.9
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.000 206.1
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 0 0> 0.000 106.0
TePb (mp-19717) <1 1 1> <1 1 1> 0.001 298.3
TePb (mp-19717) <1 0 0> <1 0 0> 0.001 172.2
GaAs (mp-2534) <1 0 0> <1 0 0> 0.002 66.2
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.005 168.6
Ge (mp-32) <1 0 0> <1 0 0> 0.005 66.2
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.005 119.2
Si (mp-149) <1 1 0> <1 1 0> 0.006 168.6
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.007 206.1
Si (mp-149) <1 0 0> <1 0 0> 0.007 119.2
CdS (mp-672) <1 1 0> <1 1 0> 0.007 149.9
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.008 68.8
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.008 22.9
C (mp-48) <0 0 1> <1 1 1> 0.011 68.8
InP (mp-20351) <1 1 0> <1 1 0> 0.011 149.9
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.012 66.2
Fe2O3 (mp-24972) <1 0 1> <1 0 0> 0.019 225.2
BaF2 (mp-1029) <1 1 1> <1 1 1> 0.025 68.8
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.026 56.2
LaF3 (mp-905) <1 0 1> <1 0 0> 0.026 212.0
LiF (mp-1138) <1 0 0> <1 0 0> 0.030 66.2
Al (mp-134) <1 1 0> <1 1 0> 0.031 206.1
Te2W (mp-22693) <1 1 0> <1 1 0> 0.036 112.4
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.039 66.2
C (mp-48) <1 0 0> <1 0 0> 0.041 172.2
Fe2O3 (mp-24972) <1 0 0> <1 0 0> 0.044 212.0
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.047 225.2
Ge (mp-32) <1 1 0> <1 0 0> 0.065 331.2
WS2 (mp-224) <1 0 0> <1 1 0> 0.071 224.8
TiO2 (mp-2657) <1 1 1> <1 1 0> 0.076 206.1
LiGaO2 (mp-5854) <1 1 1> <1 1 1> 0.076 275.4
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.087 56.2
Cu (mp-30) <1 1 1> <1 1 1> 0.089 22.9
Cu (mp-30) <1 1 0> <1 1 0> 0.093 18.7
Cu (mp-30) <1 0 0> <1 0 0> 0.105 13.2
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.111 149.9
AlN (mp-661) <1 0 1> <1 0 0> 0.114 198.7
GaTe (mp-542812) <1 0 0> <1 1 0> 0.116 224.8
GaAs (mp-2534) <1 1 0> <1 0 0> 0.117 331.2
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.118 131.2
NdGaO3 (mp-3196) <1 0 1> <1 1 0> 0.121 318.5
Au (mp-81) <1 1 1> <1 1 1> 0.122 91.8
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.124 168.6
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.126 53.0
Au (mp-81) <1 1 0> <1 1 0> 0.127 74.9
ZnO (mp-2133) <1 1 0> <1 1 0> 0.133 337.2
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.134 160.6
YVO4 (mp-19133) <1 0 1> <1 0 0> 0.135 212.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
298 41 41 0 0 0
41 298 41 0 0 0
41 41 298 0 0 0
0 0 0 54 0 0
0 0 0 0 54 0
0 0 0 0 0 54
Compliance Tensor Sij (10-12Pa-1)
3.5 -0.4 -0.4 0 0 0
-0.4 3.5 -0.4 0 0 0
-0.4 -0.4 3.5 0 0 0
0 0 0 18.5 0 0
0 0 0 0 18.5 0
0 0 0 0 0 18.5
Shear Modulus GV
84 GPa
Bulk Modulus KV
126 GPa
Shear Modulus GR
70 GPa
Bulk Modulus KR
126 GPa
Shear Modulus GVRH
77 GPa
Bulk Modulus KVRH
126 GPa
Elastic Anisotropy
0.95
Poisson's Ratio
0.25

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
1.90 -0.00 0.00
-0.00 1.90 -0.00
0.00 -0.00 1.90
Dielectric Tensor εij (total)
4.93 -0.00 0.00
-0.00 4.93 -0.00
0.00 -0.00 4.93
Polycrystalline dielectric constant εpoly
(electronic contribution)
1.90
Polycrystalline dielectric constant εpoly
(total)
4.93
Refractive Index n
1.38
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ReWO6 (mvc-5744) 0.0698 0.022 3
ZrFeF6 (mp-608332) 0.1104 0.174 3
TeWO6 (mvc-5676) 0.0327 0.059 3
ZrCoF6 (mp-555491) 0.1103 0.141 3
ZrFeF6 (mp-554971) 0.1104 0.174 3
CoAg3(CN)6 (mp-6573) 0.6731 0.236 4
CdPd(CN)6 (mp-606650) 0.5961 0.368 4
FeAg3(CN)6 (mp-568663) 0.6965 0.307 4
CrO3 (mvc-11943) 0.1103 0.400 2
CoF3 (mp-559435) 0.0175 0.005 2
FeF3 (mp-558852) 0.0555 0.011 2
CoF3 (mp-603815) 0.0807 0.005 2
FeF3 (mp-603849) 0.0373 0.011 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al F
Final Energy/Atom
-5.8932 eV
Corrected Energy
-23.5729 eV
-23.5729 eV = -23.5729 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 252641
  • 252640
  • 252643
  • 252642
  • 130021
Submitted by
User remarks:
  • Aluminium fluoride - alpha

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)