Final Magnetic Moment0.863 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.376 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.014 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTi3O5 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 344.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 187.8 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 267.6 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 106.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 150.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 150.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 338.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 263.0 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 321.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 263.0 |
Al (mp-134) | <1 1 0> | <0 0 1> | 338.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 112.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 263.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 305.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 263.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 187.8 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 338.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 150.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 106.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 112.7 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 213.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 263.0 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 344.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 112.7 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 338.1 |
SiC (mp-7631) | <1 0 0> | <0 1 1> | 268.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 338.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 338.1 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 1> | 214.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 338.1 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 213.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 112.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 300.5 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 263.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 268.0 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 268.0 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 213.0 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 191.2 |
TiO2 (mp-2657) | <0 0 1> | <0 1 1> | 268.0 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 150.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 300.5 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 267.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 300.5 |
C (mp-66) | <1 1 0> | <0 0 1> | 225.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 263.0 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 268.0 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 299.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 150.3 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 1> | 106.5 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 112.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgTi11O20 (mp-766100) | 0.1920 | 0.018 | 3 |
MgTi23O40 (mp-760088) | 0.2316 | 0.017 | 3 |
Al2CrO5 (mp-770006) | 0.2620 | 0.038 | 3 |
TiAl2O5 (mp-4930) | 0.2329 | 0.013 | 3 |
MgTi14O25 (mp-774738) | 0.2249 | 0.018 | 3 |
LiCo2O2F3 (mp-850987) | 0.4717 | 0.303 | 4 |
LiMn2O2F3 (mp-765996) | 0.3823 | 0.023 | 4 |
LiV2O2F3 (mp-765853) | 0.4587 | 0.066 | 4 |
LiV2O2F3 (mp-765822) | 0.4163 | 0.268 | 4 |
LiFe2O2F3 (mp-774121) | 0.4020 | 0.070 | 4 |
Ta3N5 (mp-27488) | 0.2554 | 0.000 | 2 |
Nb3N5 (mp-754556) | 0.3282 | 0.018 | 2 |
Ti6O11 (mp-559964) | 0.5970 | 0.008 | 2 |
Ti3O5 (mp-556480) | 0.2126 | 0.009 | 2 |
Ti4O7 (mp-12205) | 0.6277 | 0.005 | 2 |
Li4NbFe(WO6)2 (mp-850102) | 0.6389 | 0.019 | 5 |
Li4MnNb(WO6)2 (mp-771868) | 0.5841 | 0.027 | 5 |
Li4FeBi(TeO6)2 (mp-776005) | 0.6465 | 0.035 | 5 |
Li4VFe(TeO6)2 (mp-761819) | 0.6371 | 0.060 | 5 |
Li4MnV2WO12 (mp-773239) | 0.6398 | 0.089 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv O |
Final Energy/Atom-8.9899 eV |
Corrected Energy-150.8606 eV
-150.8606 eV = -143.8377 eV (uncorrected energy) - 7.0229 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)