Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.179 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.05 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 128.1 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 128.1 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 0> | 128.1 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 274.6 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 128.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 294.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 256.2 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 113.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 113.2 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 128.1 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 156.9 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 196.1 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 96.1 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 352.3 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 274.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 203.8 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 274.6 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 156.9 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 274.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 339.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 271.8 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 274.6 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 196.1 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 96.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 96.1 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 294.4 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 224.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 96.1 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 117.7 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 256.2 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 256.2 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 64.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 256.2 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 288.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 203.8 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 224.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 196.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 274.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 181.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 117.7 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 113.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 196.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 117.7 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 96.1 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 203.8 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 196.1 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 117.7 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 294.4 |
Te2W (mp-22693) | <1 1 1> | <1 1 0> | 224.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 156.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
53 | 43 | 43 | 0 | 0 | 0 |
43 | 53 | 43 | 0 | 0 | 0 |
43 | 43 | 53 | 0 | 0 | 0 |
0 | 0 | 0 | 18 | 0 | 0 |
0 | 0 | 0 | 0 | 18 | 0 |
0 | 0 | 0 | 0 | 0 | 18 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
64.3 | -28.5 | -28.5 | 0 | 0 | 0 |
-28.5 | 64.3 | -28.5 | 0 | 0 | 0 |
-28.5 | -28.5 | 64.3 | 0 | 0 | 0 |
0 | 0 | 0 | 55.5 | 0 | 0 |
0 | 0 | 0 | 0 | 55.5 | 0 |
0 | 0 | 0 | 0 | 0 | 55.5 |
Shear Modulus GV13 GPa |
Bulk Modulus KV46 GPa |
Shear Modulus GR9 GPa |
Bulk Modulus KR46 GPa |
Shear Modulus GVRH11 GPa |
Bulk Modulus KVRH46 GPa |
Elastic Anisotropy1.97 |
Poisson's Ratio0.39 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.000 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.180 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
ZrHg3 (mp-1608) | 0.0000 | 0.024 | 2 |
YGa3 (mp-979423) | 0.0000 | 0.000 | 2 |
UTl3 (mp-21844) | 0.0000 | 0.212 | 2 |
LiAl3 (mp-10890) | 0.0000 | 0.000 | 2 |
DyTl3 (mp-2415) | 0.0000 | 0.000 | 2 |
Na (mp-974558) | 0.0000 | 0.001 | 1 |
Br (mp-998870) | 0.0000 | 0.666 | 1 |
Mn (mp-8634) | 0.0000 | 0.083 | 1 |
Pb (mp-20483) | 0.0000 | 0.000 | 1 |
Cu (mp-30) | 0.0000 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 Tl_d |
Final Energy/Atom-3.0691 eV |
Corrected Energy-12.2762 eV
-12.2762 eV = -12.2762 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)