Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.930 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.294 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 -1 1> | 256.9 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 298.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 298.4 |
AlN (mp-661) | <1 1 0> | <0 1 -1> | 326.4 |
CeO2 (mp-20194) | <1 1 1> | <1 -1 1> | 256.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 298.4 |
GaN (mp-804) | <0 0 1> | <0 1 -1> | 326.4 |
GaN (mp-804) | <1 0 1> | <1 -1 0> | 250.4 |
GaN (mp-804) | <1 1 1> | <1 -1 -1> | 267.2 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 233.2 |
CeO2 (mp-20194) | <1 0 0> | <1 -1 -1> | 267.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 133.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 233.2 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 291.5 |
SiO2 (mp-6930) | <1 1 0> | <0 1 -1> | 195.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 119.4 |
GaN (mp-804) | <1 1 0> | <0 1 -1> | 326.4 |
SiO2 (mp-6930) | <1 0 0> | <1 1 -1> | 273.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 291.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 -1> | 273.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 222.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 233.2 |
ZnSe (mp-1190) | <1 1 1> | <0 1 -1> | 326.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 311.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 133.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 133.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 226.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 222.5 |
CdS (mp-672) | <1 0 1> | <1 -1 1> | 256.9 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 291.5 |
CdS (mp-672) | <1 0 0> | <1 -1 -1> | 267.2 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 263.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 174.9 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 267.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 133.5 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 291.5 |
YVO4 (mp-19133) | <1 1 1> | <1 -1 0> | 250.4 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 273.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 267.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 174.9 |
Te2Mo (mp-602) | <1 0 1> | <1 -1 -1> | 267.2 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 226.0 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 291.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 222.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 -1> | 261.1 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 133.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 267.1 |
BN (mp-984) | <1 1 1> | <0 1 0> | 273.3 |
BN (mp-984) | <1 0 0> | <1 -1 -1> | 133.6 |
BN (mp-984) | <1 0 1> | <1 1 -1> | 182.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
5.42 | 0.21 | -0.29 |
0.21 | 5.45 | -0.19 |
-0.29 | -0.19 | 6.23 |
Dielectric Tensor εij (total) |
||
---|---|---|
16.80 | 3.76 | 1.40 |
3.76 | 13.91 | -1.12 |
1.40 | -1.12 | 22.52 |
Polycrystalline dielectric constant
εpoly∞
5.70
|
Polycrystalline dielectric constant
εpoly
17.75
|
Refractive Index n2.39 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tl2GeS3 (mp-7277) | 0.2503 | 0.000 | 3 |
Ba5(SiN3)2 (mp-29060) | 0.5379 | 0.015 | 3 |
Cs4Ga2Se5 (mp-574485) | 0.4428 | 0.001 | 3 |
Tl2SiSe3 (mp-14241) | 0.2244 | 0.000 | 3 |
Tl2GeSe3 (mp-14242) | 0.3713 | 0.000 | 3 |
CsGeBiS4 (mp-553970) | 0.5992 | 0.000 | 4 |
NaSb(PS3)2 (mp-554384) | 0.5802 | 0.001 | 4 |
K2Hg(PSe3)2 (mp-568855) | 0.6071 | 0.000 | 4 |
K2Ge2PbS6 (mp-561132) | 0.5202 | 0.000 | 4 |
AgBi(PS3)2 (mp-556434) | 0.6133 | 0.000 | 4 |
GaI2 (mp-570738) | 0.6545 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d Si S |
Final Energy/Atom-4.3574 eV |
Corrected Energy-55.3070 eV
Uncorrected energy = -52.2890 eV
Composition-based energy adjustment (-0.503 eV/atom x 6.0 atoms) = -3.0180 eV
Corrected energy = -55.3070 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)