material

Sr(CdP)2

ID:

mp-8277

DOI:

10.17188/1308008


Tags: Dicadmium strontium diphosphide Strontium dicadmium phosphide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.595 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.08 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.710 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 30912 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdSe (mp-2691) <1 0 0> <1 0 0> 0.001 193.1
CdSe (mp-2691) <1 1 1> <0 0 1> 0.002 66.7
GaSb (mp-1156) <1 0 0> <1 0 0> 0.003 193.1
GaN (mp-804) <0 0 1> <0 0 1> 0.004 116.8
TiO2 (mp-390) <1 0 1> <0 0 1> 0.006 317.0
GaSb (mp-1156) <1 1 1> <0 0 1> 0.008 66.7
PbSe (mp-2201) <1 0 0> <1 0 0> 0.010 193.1
CdS (mp-672) <0 0 1> <0 0 1> 0.012 200.2
C (mp-66) <1 1 1> <0 0 1> 0.013 66.7
Fe3O4 (mp-19306) <1 0 0> <1 1 1> 0.014 290.9
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.017 66.7
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.017 66.7
TiO2 (mp-390) <0 0 1> <1 1 1> 0.018 58.2
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.020 66.7
SiC (mp-8062) <1 0 0> <1 0 0> 0.021 96.5
TiO2 (mp-2657) <1 0 0> <1 0 1> 0.022 290.0
PbSe (mp-2201) <1 1 1> <0 0 1> 0.022 66.7
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.027 66.7
LiGaO2 (mp-5854) <1 0 1> <1 0 1> 0.028 181.2
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.030 253.7
WSe2 (mp-1821) <1 0 1> <1 0 1> 0.034 253.7
InAs (mp-20305) <1 1 1> <0 0 1> 0.035 66.7
GaSe (mp-1943) <0 0 1> <0 0 1> 0.041 50.0
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.042 193.1
PbS (mp-21276) <1 0 0> <1 1 1> 0.045 290.9
C (mp-66) <1 0 0> <0 0 1> 0.046 266.9
MgAl2O4 (mp-3536) <1 1 1> <0 0 1> 0.051 116.8
InAs (mp-20305) <1 0 0> <1 0 0> 0.052 193.1
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.053 350.3
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.060 250.2
LiF (mp-1138) <1 1 1> <0 0 1> 0.061 116.8
Te2W (mp-22693) <0 1 1> <1 0 1> 0.066 290.0
SiO2 (mp-6930) <1 1 0> <1 0 1> 0.071 145.0
TiO2 (mp-2657) <1 1 1> <1 0 1> 0.073 145.0
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.076 200.2
SiC (mp-7631) <1 0 0> <1 1 1> 0.079 232.7
LaF3 (mp-905) <1 1 0> <1 1 0> 0.083 278.7
Mg (mp-153) <1 0 1> <1 0 0> 0.089 225.2
MgO (mp-1265) <1 1 1> <0 0 1> 0.089 216.9
MgO (mp-1265) <1 0 0> <1 1 1> 0.090 232.7
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.090 250.2
WS2 (mp-224) <1 0 1> <1 0 0> 0.093 321.8
BN (mp-984) <1 0 1> <0 0 1> 0.096 183.5
YVO4 (mp-19133) <1 1 1> <1 0 1> 0.099 253.7
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.102 350.3
SiC (mp-11714) <1 0 0> <1 0 1> 0.109 253.7
SiO2 (mp-6930) <1 1 1> <0 0 1> 0.112 266.9
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.116 278.7
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.123 278.7
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.123 225.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
108 32 29 -2 0 0
32 108 29 2 0 0
29 29 89 0 0 0
-2 2 0 31 0 0
0 0 0 0 31 -2
0 0 0 0 -2 38
Compliance Tensor Sij (10-12Pa-1)
10.7 -2.5 -2.7 0.6 0 0
-2.5 10.7 -2.7 -0.6 0 0
-2.7 -2.7 12.9 0 0 0
0.6 -0.6 0 32.5 0 0
0 0 0 0 32.5 1.3
0 0 0 0 1.3 26.4
Shear Modulus GV
34 GPa
Bulk Modulus KV
54 GPa
Shear Modulus GR
34 GPa
Bulk Modulus KR
53 GPa
Shear Modulus GVRH
34 GPa
Bulk Modulus KVRH
53 GPa
Elastic Anisotropy
0.07
Poisson's Ratio
0.24

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
12.65 -0.00 0.00
-0.00 12.65 0.00
0.00 0.00 10.79
Dielectric Tensor εij (total)
20.78 -0.00 0.00
-0.00 20.77 0.00
0.00 0.00 25.74
Polycrystalline dielectric constant εpoly
(electronic contribution)
12.03
Polycrystalline dielectric constant εpoly
(total)
22.43
Refractive Index n
3.47
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ca(MgAs)2 (mp-9564) 0.0961 0.000 3
Sr(CdAs)2 (mp-7771) 0.0730 0.000 3
Sr(CdSb)2 (mp-7432) 0.0818 0.000 3
Yb(ZnAs)2 (mp-10314) 0.0660 0.000 3
Eu(CdP)2 (mp-22609) 0.0937 0.000 3
Li6Mn(FeO3)2 (mp-764386) 0.2176 0.040 4
Li8VO5F (mp-765837) 0.7441 0.049 4
LiFeCuS2 (mp-755288) 0.2597 0.262 4
Pu2O3 (mp-908430) 0.2358 0.073 2
Mg3As2 (mp-7891) 0.2347 0.018 2
Pu2O3 (mp-21423) 0.1891 0.073 2
Ce2O3 (mp-2721) 0.2324 0.044 2
Sc2O3 (mp-13060) 0.2378 0.132 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sr_sv Cd P
Final Energy/Atom
-3.4608 eV
Corrected Energy
-17.3039 eV
Uncorrected energy = -17.3039 eV Corrected energy = -17.3039 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 30912
  • 620249
Submitted by
User remarks:
  • Strontium dicadmium phosphide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)