material

CaPd2

ID:

mp-833

DOI:

10.17188/1308039


Tags: Calcium palladium (1/2)

Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.694 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.21 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fd3m [227]
Hall
F 4d 2 3 1d
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 58927 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiF (mp-1138) <1 0 0> <1 0 0> 0.002 300.7
BN (mp-984) <0 0 1> <1 1 1> 0.005 104.2
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.008 180.4
Si (mp-149) <1 0 0> <1 0 0> 0.018 60.1
Al (mp-134) <1 1 0> <1 1 0> 0.018 255.1
Si (mp-149) <1 1 0> <1 1 0> 0.018 85.0
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.021 60.1
Ge (mp-32) <1 0 0> <1 0 0> 0.022 300.7
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.022 85.0
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.022 85.0
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.029 255.1
TiO2 (mp-2657) <1 0 1> <1 1 0> 0.037 255.1
SiC (mp-7631) <1 0 1> <1 0 0> 0.042 240.5
GaP (mp-2490) <1 0 0> <1 0 0> 0.045 60.1
GaP (mp-2490) <1 1 0> <1 1 0> 0.047 85.0
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.056 255.1
GaAs (mp-2534) <1 0 0> <1 0 0> 0.066 300.7
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.083 255.1
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.090 60.1
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.095 85.0
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.105 300.7
BN (mp-984) <1 0 0> <1 1 0> 0.117 255.1
NdGaO3 (mp-3196) <0 1 1> <1 1 1> 0.117 104.2
BN (mp-984) <1 1 0> <1 1 0> 0.131 170.1
GaSe (mp-1943) <0 0 1> <1 1 0> 0.139 255.1
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.152 170.1
Au (mp-81) <1 0 0> <1 0 0> 0.164 300.7
InAs (mp-20305) <1 0 0> <1 0 0> 0.175 300.7
BN (mp-984) <1 1 1> <1 0 0> 0.176 240.5
LiF (mp-1138) <1 1 0> <1 1 0> 0.184 255.1
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.192 60.1
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.192 255.1
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.199 300.7
TiO2 (mp-390) <1 0 0> <1 0 0> 0.214 300.7
ZnO (mp-2133) <1 1 1> <1 1 0> 0.239 255.1
C (mp-48) <1 0 0> <1 1 0> 0.245 170.1
KCl (mp-23193) <1 1 0> <1 1 0> 0.269 170.1
SiC (mp-8062) <1 0 0> <1 0 0> 0.269 300.7
MgO (mp-1265) <1 0 0> <1 0 0> 0.271 240.5
Ag (mp-124) <1 0 0> <1 0 0> 0.283 300.7
TeO2 (mp-2125) <0 0 1> <1 1 0> 0.290 255.1
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.303 300.7
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.333 300.7
Al (mp-134) <1 0 0> <1 0 0> 0.342 300.7
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.347 240.5
TeO2 (mp-2125) <0 1 1> <1 0 0> 0.356 300.7
LaAlO3 (mp-2920) <1 0 1> <1 0 0> 0.367 300.7
SiC (mp-7631) <1 0 0> <1 0 0> 0.383 240.5
InSb (mp-20012) <1 1 0> <1 1 0> 0.390 255.1
C (mp-48) <0 0 1> <1 0 0> 0.410 300.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
130 76 76 0 0 0
76 130 76 0 0 0
76 76 130 0 0 0
0 0 0 46 0 0
0 0 0 0 46 0
0 0 0 0 0 46
Compliance Tensor Sij (10-12Pa-1)
13.5 -5 -5 0 0 0
-5 13.5 -5 0 0 0
-5 -5 13.5 0 0 0
0 0 0 21.9 0 0
0 0 0 0 21.9 0
0 0 0 0 0 21.9
Shear Modulus GV
38 GPa
Bulk Modulus KV
94 GPa
Shear Modulus GR
36 GPa
Bulk Modulus KR
94 GPa
Shear Modulus GVRH
37 GPa
Bulk Modulus KVRH
94 GPa
Elastic Anisotropy
0.33
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
YbNi4Au (mp-1024977) 0.0000 0.040 3
TmInCu4 (mp-1024957) 0.0028 0.000 3
GdNi4Au (mp-1077131) 0.0027 0.855 3
YbCu4Au (mp-1077165) 0.0028 0.000 3
GdInCu4 (mp-1077293) 0.0009 0.000 3
EuIr2 (mp-995) 0.0000 0.000 2
HfNi2 (mp-30708) 0.0000 0.048 2
Mg2Ge (mp-250) 0.0000 0.483 2
ThAl2 (mp-16720) 0.0000 0.035 2
SmPt2 (mp-1127) 0.0000 0.000 2
Co (mp-1072089) 0.0000 0.199 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Pd
Final Energy/Atom
-4.8159 eV
Corrected Energy
-28.8955 eV
-28.8955 eV = -28.8955 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 619495
  • 58927
Submitted by
User remarks:
  • Calcium palladium (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)