material

SiO2

ID:

mp-8352

DOI:

10.17188/1281939


Tags: Silicon oxide Cristobalite beta high Cristobalite high Cristobalite beta

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.266 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.012 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
1.92 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
SiO2
Band Gap
5.467 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fd3m [227]
Hall
F 4d 2 3 1d
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 35536 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Cu (mp-30) <1 0 0> <1 0 0> 0.002 222.7
Cu (mp-30) <1 1 0> <1 1 0> 0.002 314.9
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.005 278.3
ZrO2 (mp-2858) <1 0 -1> <1 1 1> 0.006 289.2
Al (mp-134) <1 0 0> <1 0 0> 0.011 278.3
ZnO (mp-2133) <0 0 1> <1 1 1> 0.016 289.2
Ni (mp-23) <1 0 0> <1 0 0> 0.022 111.3
Ni (mp-23) <1 1 0> <1 1 0> 0.024 157.4
C (mp-66) <1 1 1> <1 1 1> 0.026 289.2
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.029 55.7
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.038 289.2
ZnO (mp-2133) <1 0 0> <1 0 0> 0.041 278.3
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.043 222.7
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.049 278.3
Mg (mp-153) <1 0 0> <1 0 0> 0.052 167.0
LaF3 (mp-905) <1 1 0> <1 0 0> 0.056 278.3
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.082 236.2
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.092 55.7
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.092 111.3
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.093 96.4
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.095 314.9
Ag (mp-124) <1 0 0> <1 0 0> 0.096 222.7
GaN (mp-804) <0 0 1> <1 1 0> 0.098 314.9
SiO2 (mp-6930) <1 1 1> <1 1 0> 0.111 157.4
GaN (mp-804) <1 1 0> <1 1 0> 0.119 236.2
InSb (mp-20012) <1 0 0> <1 0 0> 0.121 222.7
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.124 78.7
PbS (mp-21276) <1 1 1> <1 1 0> 0.138 314.9
CdTe (mp-406) <1 0 0> <1 0 0> 0.147 222.7
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.170 314.9
ZrO2 (mp-2858) <1 0 0> <1 1 1> 0.194 289.2
Au (mp-81) <1 0 0> <1 0 0> 0.214 222.7
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.220 278.3
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.250 55.7
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.262 334.0
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.262 334.0
NdGaO3 (mp-3196) <0 0 1> <1 0 0> 0.263 278.3
TiO2 (mp-390) <1 0 1> <1 1 0> 0.269 78.7
ZnTe (mp-2176) <1 1 1> <1 0 0> 0.279 334.0
CdS (mp-672) <0 0 1> <1 0 0> 0.289 278.3
InAs (mp-20305) <1 1 1> <1 0 0> 0.293 334.0
GaN (mp-804) <1 0 0> <1 0 0> 0.306 167.0
Cu (mp-30) <1 1 1> <1 1 1> 0.308 289.2
LiTaO3 (mp-3666) <1 0 0> <1 1 1> 0.319 289.2
GaP (mp-2490) <1 0 0> <1 0 0> 0.325 278.3
InP (mp-20351) <1 0 0> <1 0 0> 0.335 278.3
Mg (mp-153) <1 1 0> <1 1 0> 0.339 236.2
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.346 289.2
Ni (mp-23) <1 1 1> <1 1 0> 0.367 314.9
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.370 96.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
173 114 114 0 0 0
114 173 114 0 0 0
114 114 173 0 0 0
0 0 0 81 0 0
0 0 0 0 81 0
0 0 0 0 0 81
Compliance Tensor Sij (10-12Pa-1)
12.0 -4.8 -4.8 -0.0 -0.0 -0.0
-4.8 12.0 -4.8 0.0 -0.0 -0.0
-4.8 -4.8 12.0 0.0 0.0 0.0
-0.0 0.0 0.0 12.3 -0.0 0.0
-0.0 -0.0 0.0 -0.0 12.3 0.0
-0.0 -0.0 0.0 0.0 0.0 12.3
Shear Modulus GV
61 GPa
Bulk Modulus KV
134 GPa
Shear Modulus GR
48 GPa
Bulk Modulus KR
134 GPa
Shear Modulus GVRH
54 GPa
Bulk Modulus KVRH
134 GPa
Elastic Anisotropy
1.31
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ag3AuS2 (mp-34460) 0.5437 0.000 3
Si(CN2)2 (mp-30160) 0.5290 0.028 3
Be(CN)2 (mp-35687) 0.5220 0.226 3
AlPO4 (mp-545974) 0.3363 0.011 3
Mg2ZnN2 (mp-1029265) 0.4891 1.954 3
LiB(CN)4 (mp-13590) 0.6255 0.336 4
CuB(CN)4 (mp-13589) 0.5772 0.351 4
CuCSN (mp-672285) 0.6931 0.157 4
CuCSN (mp-559044) 0.6901 0.157 4
LiCo(CO)4 (mp-18939) 0.5765 0.407 4
SiO2 (mp-7087) 0.0465 0.012 2
CrN2 (mp-1014373) 0.0022 0.342 2
Hg2N (mp-1077346) 0.0010 0.716 2
CrN2 (mp-1015780) 0.2536 0.340 2
CeSe2 (mp-1080249) 0.0014 0.528 2
C (mp-1095534) 0.6937 1.121 1
C (mp-1095633) 0.7411 0.997 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Sol-gel TiO2-SiO2 films were deposited on 316L stainless steel by dip coating process from a sono-catalysed sol of composition 30TiO2-70SiO2 prepared from a mixture of Ti(OC2H5)4 and Si(OC2H5)4, absol [...]
Bisphenol A polycarbonate (Makrolon RX 1805) from Bayer MaterialScience AG (Germany) was used as polymer matrix. A type of hydrophobic nano-SiO2 (Aerosil R8200) was chosen as filler, which was supplie [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition SiO2.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Si O
Final Energy/Atom
-7.9039 eV
Corrected Energy
-50.1711 eV
Uncorrected energy = -47.4231 eV Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV Corrected energy = -50.1711 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 77458
  • 77459
  • 77460
  • 162620
  • 35536
Submitted by
User remarks:
  • Silicon oxide
  • Cristobalite beta high