material

KYO2

ID:

mp-8409

DOI:

10.17188/1308087


Tags: High pressure experimental phase Potassium yttrium oxide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-3.107 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.02 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
3.974 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [166]
Hall
-R 3 2"
Point Group
3m
Crystal System
trigonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdSe (mp-2691) <1 1 1> <0 0 1> 0.000 200.6
GaSb (mp-1156) <1 1 1> <0 0 1> 0.003 200.6
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.003 137.2
BN (mp-984) <1 0 1> <0 0 1> 0.007 221.7
NaCl (mp-22862) <1 1 1> <0 0 1> 0.007 168.9
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.008 253.3
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.012 126.7
PbSe (mp-2201) <1 1 1> <0 0 1> 0.013 200.6
CdS (mp-672) <0 0 1> <0 0 1> 0.016 137.2
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.020 221.7
LaF3 (mp-905) <0 0 1> <0 0 1> 0.021 137.2
MgO (mp-1265) <1 0 0> <0 0 1> 0.027 200.6
C (mp-66) <1 1 1> <0 0 1> 0.029 200.6
LiF (mp-1138) <1 1 1> <0 0 1> 0.039 200.6
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.039 200.6
PbS (mp-21276) <1 0 0> <0 0 1> 0.048 253.3
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.048 337.8
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.050 200.6
MgO (mp-1265) <1 1 1> <0 0 1> 0.051 31.7
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.056 211.1
InAs (mp-20305) <1 1 1> <0 0 1> 0.062 200.6
TePb (mp-19717) <1 1 1> <0 0 1> 0.070 73.9
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.073 348.3
CdSe (mp-2691) <1 1 0> <1 0 0> 0.075 328.1
GaSb (mp-1156) <1 1 0> <1 0 0> 0.078 328.1
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.083 263.9
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.086 348.3
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.098 158.3
CdS (mp-672) <1 0 1> <0 0 1> 0.100 327.2
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.103 327.2
Te2W (mp-22693) <0 0 1> <1 0 0> 0.106 65.6
TiO2 (mp-390) <1 0 1> <1 0 0> 0.107 196.9
ZnTe (mp-2176) <1 1 0> <1 0 0> 0.109 328.1
Ge (mp-32) <1 1 0> <1 0 1> 0.111 332.3
Al (mp-134) <1 1 1> <0 0 1> 0.118 200.6
InAs (mp-20305) <1 1 0> <1 0 0> 0.119 328.1
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.129 168.9
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.136 221.7
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.137 221.7
CdWO4 (mp-19387) <1 1 0> <0 0 1> 0.159 242.8
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.161 126.7
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.163 126.7
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.166 327.2
LiGaO2 (mp-5854) <0 1 0> <1 1 0> 0.167 227.3
LiF (mp-1138) <1 1 0> <0 0 1> 0.168 211.1
GaAs (mp-2534) <1 1 0> <1 0 1> 0.170 332.3
PbS (mp-21276) <1 1 0> <0 0 1> 0.172 253.3
MgF2 (mp-1249) <1 0 1> <0 0 1> 0.174 348.3
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.178 95.0
GaAs (mp-2534) <1 1 1> <0 0 1> 0.183 168.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
188 51 30 3 0 0
51 188 30 -3 -0 0
30 30 135 0 -0 0
3 -3 0 32 0 -0
0 -0 -0 0 32 3
0 0 0 -0 3 69
Compliance Tensor Sij (10-12Pa-1)
5.9 -1.4 -1 -0.6 0 0
-1.4 5.9 -1 0.6 0 0
-1 -1 7.8 0 0 0
-0.6 0.6 0 30.9 0 0
0 0 0 0 30.9 -1.1
0 0 0 0 -1.1 14.6
Shear Modulus GV
53 GPa
Bulk Modulus KV
81 GPa
Shear Modulus GR
47 GPa
Bulk Modulus KR
78 GPa
Shear Modulus GVRH
50 GPa
Bulk Modulus KVRH
80 GPa
Elastic Anisotropy
0.76
Poisson's Ratio
0.24

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Na3Co2SbO6 (mp-19087) 0.4414 0.000 4
Na3Ni2SbO6 (mp-971678) 0.4036 0.000 4
Na3Co2SbO6 (mp-561940) 0.4951 0.098 4
Li2VO2F (mp-763175) 0.5292 0.095 4
Li2VO2F (mp-763174) 0.5507 0.096 4
Sb2Te (mp-6997) 0.3874 0.575 2
Bi2Te3 (mp-34202) 0.3839 0.000 2
Bi4Se3 (mp-27607) 0.3923 0.011 2
Te2Pd (mp-782) 0.3813 0.000 2
TlS (mp-998912) 0.3630 0.058 2
KGdO2 (mp-757021) 0.0675 0.000 3
Ca2NCl (mp-22936) 0.0293 0.000 3
RbTlO2 (mp-8176) 0.0707 0.000 3
KErO2 (mp-7959) 0.0735 0.000 3
KHoO2 (mp-754883) 0.0520 0.000 3
Xe (mp-979286) 0.7406 0.006 1
Na (mp-999501) 0.6841 0.129 1
Te (mp-570459) 0.6596 0.041 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: O K_sv Y_sv
Final Energy/Atom
-7.1160 eV
Corrected Energy
-29.8685 eV
-29.8685 eV = -28.4639 eV (uncorrected energy) - 1.4046 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 49650
Submitted by
User remarks:
  • High pressure experimental phase
  • Potassium yttrium oxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)