Final Magnetic Moment38.233 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.019 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.011 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTh2Fe7 + Fe |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <0 0 1> | 62.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 248.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 313.1 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 313.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 187.9 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 107.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 62.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 250.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 62.6 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 214.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 250.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 313.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 185.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 313.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 250.5 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 214.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 187.9 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 214.5 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 214.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 214.5 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 107.2 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 313.1 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 187.9 |
ZnTe (mp-2176) | <1 1 0> | <1 0 0> | 107.2 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 62.6 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 187.9 |
C (mp-66) | <1 1 0> | <1 0 0> | 107.2 |
LaF3 (mp-905) | <0 0 1> | <1 1 0> | 185.8 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 313.1 |
LaF3 (mp-905) | <1 1 0> | <1 1 0> | 185.8 |
PbS (mp-21276) | <1 1 0> | <1 0 1> | 248.4 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 62.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 313.1 |
InP (mp-20351) | <1 1 0> | <1 0 1> | 248.4 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 62.6 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 62.6 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 187.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 313.1 |
Ga2O3 (mp-886) | <1 0 1> | <1 1 0> | 185.8 |
Au (mp-81) | <1 0 0> | <0 0 1> | 313.1 |
WS2 (mp-224) | <1 1 1> | <0 0 1> | 250.5 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 250.5 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 250.5 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 250.5 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 187.9 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 187.9 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 250.5 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 313.1 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 313.1 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 250.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm2Cr2Fe15 (mp-3890) | 0.2099 | 0.210 | 3 |
Nd2Zn15Ge2 (mp-542178) | 0.4432 | 0.046 | 3 |
LuNi5Sn (mp-865201) | 0.7263 | 0.000 | 3 |
Pr2Fe17 (mp-880) | 0.3044 | 0.054 | 2 |
Ce2Fe17 (mp-654) | 0.3309 | 0.021 | 2 |
Nd2Co17 (mp-356) | 0.3303 | 0.000 | 2 |
Th2Fe17 (mp-843) | 0.3033 | 0.011 | 2 |
Nd2Fe17 (mp-1510) | 0.3204 | 0.322 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Th Fe_pv |
Final Energy/Atom-8.3768 eV |
Corrected Energy-159.1585 eV
-159.1585 eV = -159.1585 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)