material

Ca5(AlSb3)2

ID:

mp-8439

DOI:

10.17188/1308104


Tags: Calcium aluminium antimonide (5/2/6) Aluminium antimony calcium (2/6/5)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.771 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.24 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.218 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pbam [55]
Hall
-P 2 2ab
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiTaO3 (mp-3666) <1 1 1> <0 1 0> 0.012 127.3
CdWO4 (mp-19387) <0 1 0> <0 1 0> 0.017 318.2
LiNbO3 (mp-3731) <1 1 0> <0 1 0> 0.020 127.3
WS2 (mp-224) <0 0 1> <0 1 0> 0.068 318.2
MoS2 (mp-1434) <0 0 1> <0 1 0> 0.068 318.2
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.075 327.5
CdWO4 (mp-19387) <1 0 1> <1 0 1> 0.075 180.1
ZrO2 (mp-2858) <1 0 0> <0 1 0> 0.092 318.2
TeO2 (mp-2125) <0 1 0> <0 0 1> 0.098 272.9
GaSe (mp-1943) <1 0 1> <0 0 1> 0.098 272.9
Fe2O3 (mp-24972) <0 0 1> <0 1 0> 0.099 254.5
WS2 (mp-224) <1 0 0> <1 1 0> 0.104 183.0
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.106 272.9
LiTaO3 (mp-3666) <1 1 0> <0 1 0> 0.118 127.3
Fe2O3 (mp-24972) <1 1 1> <0 1 0> 0.135 127.3
GaN (mp-804) <1 1 1> <0 0 1> 0.138 272.9
BaF2 (mp-1029) <1 1 0> <0 1 1> 0.140 167.7
KTaO3 (mp-3614) <1 1 0> <0 1 1> 0.146 251.5
Al (mp-134) <1 1 0> <0 1 1> 0.169 251.5
Cu (mp-30) <1 1 0> <0 1 1> 0.169 167.7
TiO2 (mp-390) <1 0 0> <0 1 0> 0.180 254.5
GdScO3 (mp-5690) <1 1 1> <0 0 1> 0.181 218.3
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.192 218.3
InSb (mp-20012) <1 1 0> <0 1 1> 0.198 251.5
WS2 (mp-224) <1 1 0> <0 1 0> 0.200 318.2
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.201 272.9
ZrO2 (mp-2858) <1 1 1> <0 1 1> 0.203 251.5
Mg (mp-153) <1 1 1> <0 0 1> 0.205 272.9
LiNbO3 (mp-3731) <0 0 1> <0 1 1> 0.205 167.7
CdTe (mp-406) <1 1 0> <0 1 1> 0.211 251.5
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.224 327.5
LiNbO3 (mp-3731) <1 1 1> <0 1 0> 0.225 127.3
Cu (mp-30) <1 1 1> <0 1 0> 0.243 254.5
ZrO2 (mp-2858) <1 1 -1> <0 0 1> 0.247 272.9
MgF2 (mp-1249) <1 0 0> <0 1 0> 0.260 318.2
MgO (mp-1265) <1 1 0> <0 0 1> 0.269 327.5
LiTaO3 (mp-3666) <0 0 1> <0 1 1> 0.280 167.7
GaN (mp-804) <1 0 1> <0 0 1> 0.295 272.9
CdWO4 (mp-19387) <1 1 1> <0 1 0> 0.313 318.2
PbSe (mp-2201) <1 1 0> <0 1 1> 0.321 167.7
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.331 183.0
YAlO3 (mp-3792) <0 0 1> <0 1 0> 0.339 318.2
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.349 163.7
Au (mp-81) <1 1 0> <0 0 1> 0.352 327.5
LaAlO3 (mp-2920) <1 1 0> <0 1 1> 0.353 251.5
TbScO3 (mp-31119) <1 1 1> <0 0 1> 0.364 218.3
LaF3 (mp-905) <1 0 0> <0 1 0> 0.366 318.2
GaSb (mp-1156) <1 1 0> <0 1 1> 0.368 167.7
AlN (mp-661) <1 0 1> <0 1 0> 0.389 318.2
WS2 (mp-224) <1 0 1> <0 1 0> 0.400 318.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
71 20 20 0 0 0
20 67 27 0 0 0
20 27 82 0 0 0
0 0 0 22 0 0
0 0 0 0 18 0
0 0 0 0 0 26
Compliance Tensor Sij (10-12Pa-1)
16 -3.6 -2.8 0 0 0
-3.6 18 -5 0 0 0
-2.8 -5 14.5 0 0 0
0 0 0 45.1 0 0
0 0 0 0 55 0
0 0 0 0 0 38.8
Shear Modulus GV
23 GPa
Bulk Modulus KV
39 GPa
Shear Modulus GR
23 GPa
Bulk Modulus KR
39 GPa
Shear Modulus GVRH
23 GPa
Bulk Modulus KVRH
39 GPa
Elastic Anisotropy
0.13
Poisson's Ratio
0.25

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
13.36 0.00 0.00
0.00 16.86 0.00
0.00 0.00 15.62
Dielectric Tensor εij (total)
20.22 0.00 0.00
0.00 25.70 0.00
0.00 0.00 23.03
Polycrystalline dielectric constant εpoly
(electronic contribution)
15.28
Polycrystalline dielectric constant εpoly
(total)
22.98
Refractive Index n
3.91
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ba5(InSb3)2 (mp-615760) 0.3246 0.000 3
Ca5(GaSb3)2 (mp-17985) 0.1150 0.000 3
Yb5(InSb3)2 (mp-628593) 0.3299 0.000 3
Sr5(InSb3)2 (mp-649033) 0.1699 0.000 3
Ca5(GaAs3)2 (mp-17558) 0.1888 0.000 3
HoCuPbSe3 (mp-6244) 0.6042 0.000 4
SrPrCuSe3 (mp-17660) 0.6099 0.000 4
EuDyCuS3 (mp-542765) 0.6570 0.753 4
TbCuPbSe3 (mp-601286) 0.6393 0.000 4
BaLaCuTe3 (mp-17063) 0.6409 0.000 4
Mg5Si9 (mp-1075741) 0.7076 0.202 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Al Sb
Final Energy/Atom
-4.0240 eV
Corrected Energy
-104.6252 eV
-104.6252 eV = -104.6252 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 60146
  • 183853
Submitted by
User remarks:
  • Aluminium antimony calcium (2/6/5)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)