material

Ca3N2

ID:

mp-844

DOI:

10.17188/1308105


Tags: Tricalcium nitride - anti-C type Calcium nitride High pressure experimental phase Calcium nitride - alpha, HT Tricalcium nitride - alpha Calcium nitride - alpha

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.933 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.61 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.111 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Ia3 [206]
Hall
-I 2b 2c 3
Point Group
m3
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdTe (mp-406) <1 1 0> <1 1 0> 0.001 186.2
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.001 186.2
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.001 131.7
InSb (mp-20012) <1 1 0> <1 1 0> 0.003 186.2
GaAs (mp-2534) <1 1 0> <1 1 0> 0.009 186.2
GaAs (mp-2534) <1 0 0> <1 0 0> 0.009 131.7
Cu (mp-30) <1 0 0> <1 0 0> 0.022 131.7
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.031 263.4
Ge (mp-32) <1 1 0> <1 1 0> 0.036 186.2
Ge (mp-32) <1 0 0> <1 0 0> 0.036 131.7
Al (mp-134) <1 1 0> <1 1 0> 0.038 186.2
Al (mp-134) <1 0 0> <1 0 0> 0.038 131.7
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.048 186.2
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.054 186.2
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.076 186.2
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.090 186.2
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.091 131.7
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.111 186.2
NaCl (mp-22862) <1 1 0> <1 1 0> 0.119 186.2
NaCl (mp-22862) <1 0 0> <1 0 0> 0.119 131.7
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.142 186.2
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.146 186.2
TePb (mp-19717) <1 1 0> <1 1 0> 0.147 186.2
ZnO (mp-2133) <1 0 0> <1 0 0> 0.218 263.4
NdGaO3 (mp-3196) <0 0 1> <1 1 0> 0.254 186.2
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.303 131.7
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.312 131.7
Mg (mp-153) <1 1 0> <1 0 0> 0.510 263.4
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.558 131.7
SrTiO3 (mp-4651) <0 0 1> <1 1 0> 0.691 186.2
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.711 131.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
113 45 45 0 0 0
45 113 45 0 0 0
45 45 113 0 0 0
0 0 0 33 0 0
0 0 0 0 33 0
0 0 0 0 0 33
Compliance Tensor Sij (10-12Pa-1)
11.4 -3.3 -3.3 -0.0 0.0 -0.0
-3.3 11.4 -3.3 0.0 -0.0 0.0
-3.3 -3.3 11.4 0.0 0.0 0.0
-0.0 0.0 0.0 30.0 0.0 -0.0
0.0 -0.0 0.0 0.0 30.0 0.0
-0.0 0.0 0.0 -0.0 0.0 30.0
Shear Modulus GV
34 GPa
Bulk Modulus KV
68 GPa
Shear Modulus GR
34 GPa
Bulk Modulus KR
68 GPa
Shear Modulus GVRH
34 GPa
Bulk Modulus KVRH
68 GPa
Elastic Anisotropy
0.00
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
YTmO3 (mp-766256) 0.1615 0.003 3
Y7TmO12 (mp-766267) 0.1635 0.002 3
Y15TmO24 (mp-757001) 0.1577 0.001 3
Y13Tm3O24 (mp-766258) 0.1507 0.002 3
Y13Ho19O48 (mp-758033) 0.1627 0.000 3
LiMn7(O3F)3 (mp-765039) 0.4952 0.089 4
Mg2VWO6 (mvc-5881) 0.4802 0.022 4
Mg2TiWO6 (mvc-5939) 0.4872 0.125 4
Mg2CrWO6 (mvc-5960) 0.4812 0.670 4
InNi2SbO6 (mp-1078367) 0.4269 0.000 4
Sr3N2 (mp-986716) 0.1059 0.031 2
Fe2O3 (mp-686969) 0.1205 0.071 2
In2O3 (mp-22598) 0.1240 0.000 2
Cr2O3 (mp-776873) 0.1238 0.042 2
Sc2O3 (mp-216) 0.1028 0.000 2
Li4Fe2TeWO12 (mp-768021) 0.6502 0.085 5
Li4Mn2TeWO12 (mp-768044) 0.7126 0.058 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv N
Final Energy/Atom
-5.3270 eV
Corrected Energy
-218.8541 eV
Uncorrected energy = -213.0781 eV Composition-based energy adjustment (-0.361 eV/atom x 16.0 atoms) = -5.7760 eV Corrected energy = -218.8541 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 169725
  • 410754
  • 162791
  • 34678
  • 50991
Submitted by
User remarks:
  • Tricalcium nitride - anti-C type
  • High pressure experimental phase

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)