Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.694 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2MnSiO4 |
Band Gap2.964 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 224.3 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 35.1 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 128.5 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 226.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 28.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 44.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 105.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 276.7 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 105.4 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 224.0 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 307.9 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 251.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 224.3 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 224.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 259.2 |
CdS (mp-672) | <0 0 1> | <1 0 -1> | 140.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 226.8 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 128.5 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 259.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 84.0 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 32.4 |
AlN (mp-661) | <1 0 1> | <1 1 -1> | 143.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 28.0 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 175.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 134.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 259.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 175.7 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 226.8 |
Te2W (mp-22693) | <1 0 0> | <1 1 -1> | 95.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 89.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 84.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 134.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 276.7 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 256.9 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 140.5 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 64.8 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 210.8 |
TePb (mp-19717) | <1 1 1> | <1 0 -1> | 316.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 140.5 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 162.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 226.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 134.6 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 198.0 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 324.0 |
GaN (mp-804) | <1 0 0> | <1 1 -1> | 239.0 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 140.5 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 210.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 140.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 140.0 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 162.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3AsO4 (mp-9197) | 0.2422 | 0.000 | 3 |
Li3CrO4 (mp-770632) | 0.2328 | 0.000 | 3 |
Li3VS4 (mp-755642) | 0.2446 | 0.037 | 3 |
Li3VO4 (mp-19219) | 0.2584 | 0.000 | 3 |
Li3PO4 (mp-13725) | 0.1457 | 0.000 | 3 |
Li2FeSiO4 (mp-764346) | 0.1000 | 0.217 | 4 |
Li2MnSiO4 (mp-566680) | 0.1016 | 0.000 | 4 |
Li2FeSiO4 (mp-18968) | 0.0958 | 0.000 | 4 |
Li2MnSiO4 (mp-768020) | 0.0916 | 0.020 | 4 |
Li2FeSiO4 (mp-763629) | 0.0958 | 0.004 | 4 |
ZnP2 (mp-2782) | 0.5130 | 0.000 | 2 |
Si3H (mp-995193) | 0.5390 | 0.032 | 2 |
ZnP2 (mp-11025) | 0.5148 | 0.000 | 2 |
FeO (mp-781777) | 0.5360 | 0.947 | 2 |
Si3H (mp-1040468) | 0.5347 | 0.044 | 2 |
Si (mp-1079297) | 0.6716 | 0.072 | 1 |
Si (mp-971661) | 0.5639 | 0.080 | 1 |
C (mp-1078845) | 0.5829 | 0.266 | 1 |
C (mp-1080826) | 0.6189 | 0.299 | 1 |
Si (mp-1095269) | 0.6548 | 0.094 | 1 |
Explore more synthesis descriptions for materials of composition Li2MnSiO4.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Si O |
Final Energy/Atom-6.9074 eV |
Corrected Energy-238.7000 eV
Uncorrected energy = -221.0360 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-1.668 eV/atom x 4.0 atoms) = -6.6720 eV
Corrected energy = -238.7000 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)