Final Magnetic Moment2.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.736 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.035 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVPO4F + Li3PO4 + V4P3 + V2O3 + LiF |
Band Gap2.721 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 202.6 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 135.1 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 164.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 200.3 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 200.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 66.8 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 115.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 200.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 267.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 267.0 |
BN (mp-984) | <1 0 0> | <1 0 1> | 115.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 267.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 272.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 267.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 200.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 200.3 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 231.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 267.0 |
Al (mp-134) | <1 0 0> | <1 0 -1> | 272.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 136.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 66.8 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 133.5 |
C (mp-66) | <1 0 0> | <1 0 0> | 202.6 |
MgO (mp-1265) | <1 1 1> | <1 0 -1> | 272.1 |
GaP (mp-2490) | <1 1 1> | <1 0 0> | 202.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 200.3 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 267.0 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 66.8 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 115.8 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 1> | 190.1 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 270.2 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 267.0 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 267.0 |
Si (mp-149) | <1 1 1> | <0 0 1> | 200.3 |
Au (mp-81) | <1 1 1> | <0 0 1> | 267.0 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 133.5 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 200.3 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 267.0 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 267.0 |
SiC (mp-11714) | <1 1 1> | <1 0 0> | 270.2 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 200.3 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 -1> | 136.0 |
YAlO3 (mp-3792) | <1 1 1> | <1 1 1> | 190.1 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 0> | 270.2 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 0> | 270.2 |
MgF2 (mp-1249) | <1 1 0> | <1 1 -1> | 165.4 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 200.3 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 200.3 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 1> | 115.8 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 133.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca3SiO5 (mp-558273) | 0.5698 | 0.050 | 3 |
Ca2SiO4 (mp-758006) | 0.5750 | 0.058 | 3 |
Ba3GeO5 (mp-756637) | 0.5484 | 0.034 | 3 |
Ca3SiO5 (mp-641754) | 0.5579 | 0.020 | 3 |
Ca3SiO5 (mp-554141) | 0.5318 | 0.061 | 3 |
Li2MnPO5 (mp-865136) | 0.4657 | 0.078 | 4 |
Li2VSiO5 (mp-767449) | 0.5025 | 0.052 | 4 |
Li2CrPO5 (mp-761451) | 0.4306 | 0.093 | 4 |
Na3WO4F (mp-565594) | 0.4861 | 0.004 | 4 |
CrAg3ClO4 (mp-566124) | 0.4864 | 0.022 | 4 |
Li2CrPO4F (mp-770894) | 0.4698 | 0.154 | 5 |
Li2CoPO4F (mp-770624) | 0.3899 | 0.051 | 5 |
Li2FePO4F (mp-763742) | 0.3024 | 0.032 | 5 |
Na2MnPO4F (mp-566286) | 0.3985 | 0.000 | 5 |
Li2MnPO4F (mp-771918) | 0.3217 | 0.025 | 5 |
Li3MnFeCo(PO4)3 (mp-764804) | 0.6671 | 0.030 | 6 |
Li3MnFeCo(PO4)3 (mp-764708) | 0.6579 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6662 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.6677 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6632 | 0.661 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O F |
Final Energy/Atom-6.6289 eV |
Corrected Energy-513.2082 eV
-513.2082 eV = -477.2789 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 13.4560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)