Final Magnetic Moment0.022 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-1.775 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.554 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCo3O4 + Co2SiO4 + Li2CoSiO4 + SiO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 265.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 265.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 310.1 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 274.0 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 253.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 310.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 310.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 265.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 274.0 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 112.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 354.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 310.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 221.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 253.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 221.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 310.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 354.4 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 199.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 354.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 310.1 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 354.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 274.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 310.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 265.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 310.1 |
GaSe (mp-1943) | <1 0 1> | <0 1 1> | 274.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 265.8 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 332.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 310.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 265.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 199.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 132.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 310.1 |
BN (mp-984) | <1 0 0> | <1 1 1> | 153.4 |
Al (mp-134) | <1 1 0> | <0 0 1> | 310.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 253.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 223.0 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 332.4 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 310.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 354.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 133.0 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 354.4 |
SiC (mp-7631) | <1 0 1> | <0 1 0> | 332.4 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 310.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 310.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 221.5 |
MgO (mp-1265) | <1 1 0> | <1 1 1> | 153.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 221.5 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 310.1 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 177.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
B2(CN2)3 (mp-989468) | 0.5520 | 0.437 | 3 |
Be(GaO2)2 (mp-676950) | 0.4314 | 0.116 | 3 |
Zn2SiO4 (mp-1020721) | 0.5096 | 0.111 | 3 |
Zn2SiO4 (mp-1020594) | 0.5381 | 0.010 | 3 |
Be(GaO2)2 (mp-757917) | 0.5804 | 0.000 | 3 |
LiFe3(SiO4)2 (mp-780681) | 0.3154 | 0.085 | 4 |
LiFeSiO4 (mp-762925) | 0.3154 | 0.333 | 4 |
LiFeSiO4 (mp-997531) | 0.2811 | 0.732 | 4 |
LiFeSiO4 (mp-762587) | 0.2962 | 0.066 | 4 |
LiFeSiO4 (mp-767938) | 0.3146 | 0.069 | 4 |
Cr3N4 (mp-1014369) | 0.7474 | 0.164 | 2 |
CN2 (mp-1077595) | 0.7240 | 0.691 | 2 |
Ti3N4 (mp-1080190) | 0.7221 | 0.119 | 2 |
Be3Fe4Si3SO12 (mp-627398) | 0.6402 | 0.203 | 5 |
YAl6Si18(N15O)2 (mp-677127) | 0.6202 | 0.092 | 5 |
Li4Ga3Si3IO12 (mp-557112) | 0.6435 | 0.000 | 5 |
LaAl2Si5N9O (mp-677482) | 0.5787 | 0.151 | 5 |
YAl6Si30(N15O)3 (mp-677140) | 0.6404 | 0.084 | 5 |
Na2Li2Al3Si3ClO12 (mp-43030) | 0.5180 | 0.003 | 6 |
C (mp-680372) | 0.7340 | 0.407 | 1 |
C (mp-568410) | 0.7229 | 0.507 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co Si O |
Final Energy/Atom-6.2341 eV |
Corrected Energy-295.5551 eV
-295.5551 eV = -261.8342 eV (uncorrected energy) - 16.8660 eV (MP Advanced Correction) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)