Final Magnetic Moment12.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.057 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.014 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.25 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFeSbO4 + FeSnO3 + Li2SnO3 + SnO2 |
Band Gap0.166 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Group1 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 308.2 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 200.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 61.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 200.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 275.1 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 183.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 133.8 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 267.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 214.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 246.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 126.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 267.5 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 267.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 66.9 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 200.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 308.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 61.6 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 252.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 246.6 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 91.7 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 184.9 |
BN (mp-984) | <1 0 0> | <1 0 0> | 308.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 308.2 |
BN (mp-984) | <0 0 1> | <1 0 0> | 246.6 |
BN (mp-984) | <1 1 1> | <1 0 0> | 308.2 |
Al (mp-134) | <1 0 0> | <1 0 0> | 246.6 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 91.7 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 66.9 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 184.9 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 183.4 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 133.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 275.1 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 200.7 |
C (mp-66) | <1 1 0> | <0 0 1> | 267.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 267.5 |
C (mp-66) | <1 0 0> | <0 0 1> | 267.5 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 1> | 126.3 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 66.9 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 0> | 214.3 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 133.8 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 267.5 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 1> | 126.3 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 0> | 214.3 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 308.2 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 267.5 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 267.5 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 200.7 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 308.2 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 1> | 252.6 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 66.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(FeO2)2 (mp-771571) | 0.2982 | 0.074 | 3 |
Li7W5O16 (mp-771579) | 0.2370 | 0.058 | 3 |
Ca(MoO2)2 (mvc-6227) | 0.2479 | 0.222 | 3 |
Ca(FeO2)2 (mvc-6160) | 0.2896 | 0.119 | 3 |
Zn7(SbO6)2 (mp-675797) | 0.2974 | 0.009 | 3 |
Li4V5Fe3O16 (mp-776768) | 0.2345 | 0.052 | 4 |
Li7Fe3(WO8)2 (mp-771510) | 0.2418 | 0.089 | 4 |
Li4Fe5Sb3O16 (mp-770140) | 0.2304 | 0.040 | 4 |
Li4V5Cr3O16 (mp-777002) | 0.2331 | 0.027 | 4 |
Li4Nb5Cr3O16 (mp-771179) | 0.2440 | 0.104 | 4 |
Fe3O4 (mp-715491) | 0.4513 | 0.015 | 2 |
Ge3N4 (mp-641541) | 0.4632 | 0.208 | 2 |
Mn3N4 (mp-1080204) | 0.4516 | 0.073 | 2 |
Cr3N4 (mp-1014358) | 0.4326 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.4259 | 0.057 | 2 |
Li4Ti2Cr3Sn3O16 (mp-776772) | 0.1850 | 0.076 | 5 |
Li4Co3Sn3(SbO8)2 (mp-776826) | 0.1072 | 0.018 | 5 |
Li4Ti3Mn3V2O16 (mp-770420) | 0.1515 | 0.087 | 5 |
Li4Ni3Sn3(SbO8)2 (mp-777462) | 0.1471 | 0.024 | 5 |
Li4Mn3Nb2Sn3O16 (mp-762659) | 0.1786 | 0.042 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6801 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764708) | 0.6954 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6924 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.6963 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6926 | 0.661 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Sn_d Sb O |
Final Energy/Atom-6.0947 eV |
Corrected Energy-380.1735 eV
-380.1735 eV = -341.3022 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 16.3980 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)