Final Magnetic Moment15.094 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.538 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.070 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2CoSiO4 + Li(CoO2)2 + SiO2 |
Band Gap0.178 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 -1> | 277.4 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 283.2 |
AlN (mp-661) | <0 0 1> | <1 -1 -1> | 193.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 302.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 75.7 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 126.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 151.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 201.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 327.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 277.5 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 193.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 201.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 50.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 252.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 327.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 277.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 151.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 126.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 151.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 277.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 327.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 176.6 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 302.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 302.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 201.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 327.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 277.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 327.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 353.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 252.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 176.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 227.0 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 182.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 277.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 327.9 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 201.8 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 176.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 126.1 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 302.7 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 283.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 283.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 276.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 289.5 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 289.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 201.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 252.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 227.0 |
BN (mp-984) | <1 1 1> | <0 1 0> | 273.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 353.1 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 184.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr5(Si2O7)2 (mp-767345) | 0.6271 | 0.100 | 3 |
MgSiO3 (mp-642210) | 0.5920 | 0.165 | 3 |
LiPO3 (mp-29195) | 0.6968 | 0.000 | 3 |
Li2CrO4 (mp-769803) | 0.5950 | 0.070 | 3 |
V2Zn4O9 (mp-504923) | 0.7106 | 0.019 | 3 |
Li2Fe2Si3O10 (mp-767726) | 0.3762 | 0.173 | 4 |
Li3Co2Si3O10 (mp-764463) | 0.5181 | 0.178 | 4 |
Li2Mn2Si3O10 (mp-767853) | 0.5460 | 0.231 | 4 |
LiFeSiO4 (mp-762686) | 0.5277 | 0.088 | 4 |
LiNiPO4 (mp-772673) | 0.5419 | 0.058 | 4 |
NaLiZnP2O7 (mp-676483) | 0.6807 | 0.002 | 5 |
K2Mn2Zn4Si4O15 (mp-567173) | 0.7108 | 0.004 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co Si O |
Final Energy/Atom-6.7642 eV |
Corrected Energy-257.0406 eV
Uncorrected energy = -236.7486 eV
Composition-based energy adjustment (-0.687 eV/atom x 20.0 atoms) = -13.7400 eV
Composition-based energy adjustment (-1.638 eV/atom x 4.0 atoms) = -6.5520 eV
Corrected energy = -257.0406 eV
|