Final Magnetic Moment35.024 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.543 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.074 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnPO4 + Mn3(PO4)2 |
Band Gap2.906 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 0> | 238.1 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 289.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 279.3 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 209.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 209.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 289.4 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 279.3 |
CdS (mp-672) | <1 0 0> | <1 1 -1> | 175.2 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 96.5 |
BN (mp-984) | <0 0 1> | <0 1 0> | 279.3 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 192.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 209.5 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 279.3 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 279.3 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 96.5 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 289.4 |
C (mp-66) | <1 1 0> | <1 0 0> | 289.4 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 0> | 209.5 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 0> | 289.4 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 279.3 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 209.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 157.9 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 157.9 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 289.4 |
TiO2 (mp-390) | <1 0 1> | <0 1 0> | 279.3 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 279.3 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 209.5 |
GaSb (mp-1156) | <1 1 0> | <0 1 0> | 279.3 |
SrTiO3 (mp-4651) | <1 0 1> | <0 1 0> | 209.5 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 157.9 |
Cu (mp-30) | <1 1 0> | <0 1 0> | 279.3 |
Al2O3 (mp-1143) | <1 0 0> | <1 0 0> | 192.9 |
ZnTe (mp-2176) | <1 1 0> | <0 1 0> | 279.3 |
TbScO3 (mp-31119) | <0 1 1> | <0 1 0> | 209.5 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 0> | 289.4 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 192.9 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 279.3 |
NdGaO3 (mp-3196) | <0 1 1> | <0 1 0> | 209.5 |
NdGaO3 (mp-3196) | <1 0 1> | <0 1 0> | 209.5 |
SiC (mp-11714) | <1 1 1> | <0 1 0> | 279.3 |
Ga2O3 (mp-886) | <1 1 -1> | <1 1 0> | 238.1 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 279.3 |
WS2 (mp-224) | <1 1 0> | <0 0 1> | 157.9 |
C (mp-48) | <0 0 1> | <1 1 0> | 238.1 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 289.4 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 157.9 |
SiC (mp-8062) | <1 1 0> | <0 1 0> | 139.6 |
TiO2 (mp-390) | <1 1 0> | <0 1 0> | 209.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca(CuO2)2 (mvc-5770) | 0.6704 | 0.256 | 3 |
Fe4(PO4)3 (mp-31780) | 0.5755 | 0.020 | 3 |
Na2W2O7 (mp-25800) | 0.6551 | 0.022 | 3 |
MnSiO3 (mp-565815) | 0.6538 | 0.007 | 3 |
Sn2Ge2O7 (mp-768877) | 0.6763 | 0.039 | 3 |
Li4Fe7(PO4)6 (mp-762524) | 0.3255 | 0.062 | 4 |
Li4Cu7(PO4)6 (mp-762050) | 0.3074 | 0.094 | 4 |
Li4V7(PO4)6 (mp-763426) | 0.2315 | 0.082 | 4 |
Li4Ni7(PO4)6 (mp-32384) | 0.3503 | 0.047 | 4 |
Li4Ni7(PO4)6 (mp-687026) | 0.3189 | 0.047 | 4 |
Li3MnV(PO4)3 (mp-774311) | 0.5199 | 0.208 | 5 |
Li3MnV(PO4)3 (mp-779876) | 0.4669 | 0.219 | 5 |
Li6MnV3(PO4)6 (mp-778914) | 0.5223 | 0.027 | 5 |
Li3MnV(PO4)3 (mp-779368) | 0.5128 | 0.073 | 5 |
Li3MnV(PO4)3 (mp-779367) | 0.5226 | 0.082 | 5 |
Li4NbFe3Cu2(PO4)6 (mp-777855) | 0.6146 | 0.099 | 6 |
Li4Mn2Fe3P6WO24 (mp-770860) | 0.5831 | 0.085 | 6 |
Li4Mn2VNi3(PO4)6 (mp-770417) | 0.6172 | 0.075 | 6 |
Li4Fe2Ni3Sn(PO4)6 (mp-781476) | 0.6319 | 0.082 | 6 |
Li4TiCo2Ni3(PO4)6 (mp-778251) | 0.6289 | 0.133 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6586 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-7.2842 eV |
Corrected Energy-327.2716 eV
-327.2716 eV = -298.6507 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 11.7660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)