Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.172 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.256 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeCO3 + Li3PO4 |
Band Gap3.959 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmn21 [31] |
HallP 2ac 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 69.1 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 167.9 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 176.2 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 56.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 241.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 103.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 140.0 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 132.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 34.5 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 176.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 193.4 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 322.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 88.1 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 280.1 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 335.9 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 128.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 172.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 280.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 322.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 279.9 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 132.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 140.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 276.3 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 279.9 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 132.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 310.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 138.1 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 132.2 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 352.4 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 176.2 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 103.6 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 103.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 322.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 69.1 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 138.1 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 272.1 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 128.9 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 241.8 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 264.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 345.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 310.8 |
Te2Mo (mp-602) | <1 0 1> | <1 0 1> | 322.3 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 70.0 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 272.1 |
BN (mp-984) | <0 0 1> | <0 1 1> | 223.9 |
BN (mp-984) | <1 0 0> | <0 1 0> | 308.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 310.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 172.7 |
BN (mp-984) | <1 1 0> | <0 1 1> | 167.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 241.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiCoPO4 (mp-863861) | 0.7210 | 0.080 | 4 |
LiFeCO4 (mp-761994) | 0.7297 | 0.051 | 4 |
NaLiCO3 (mp-561310) | 0.7447 | 0.009 | 4 |
MnFeBO4 (mp-771061) | 0.7486 | 0.041 | 4 |
Li3NiAsCO7 (mp-771419) | 0.3666 | 0.047 | 5 |
Li5Fe2P2(CO7)2 (mp-770204) | 0.4153 | 0.210 | 5 |
Na3SiBiBO7 (mp-772711) | 0.4151 | 0.027 | 5 |
Li3MnPCO7 (mp-769735) | 0.1517 | 0.085 | 5 |
Li3CuSiCO7 (mp-772051) | 0.3972 | 0.085 | 5 |
Li12V3FeP4(CO7)4 (mp-767693) | 0.4591 | 0.061 | 6 |
Li12CoNi3P4(CO7)4 (mp-767857) | 0.4341 | 0.036 | 6 |
Li12VNi3P4(CO7)4 (mp-767733) | 0.4474 | 0.047 | 6 |
Na2LiMnPCO7 (mp-764273) | 0.4488 | 0.023 | 6 |
Li6VCoP2(CO7)2 (mp-767294) | 0.4366 | 0.056 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P C O |
Final Energy/Atom-6.4662 eV |
Corrected Energy-183.4193 eV
-183.4193 eV = -168.1213 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)