Final Magnetic Moment4.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.523 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.064 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMn(PO3)4 |
Band Gap1.319 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 259.6 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 200.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 251.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 324.6 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 173.0 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 282.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 259.6 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 259.6 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 -1> | 259.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 194.8 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 194.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 301.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 314.6 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 194.8 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 251.7 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 301.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 251.7 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 282.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 314.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 259.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 314.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 173.0 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 282.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 324.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 314.6 |
GaN (mp-804) | <1 1 0> | <1 1 -1> | 200.0 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 301.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 314.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 314.6 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 282.4 |
GaSe (mp-1943) | <1 0 0> | <1 1 -1> | 200.0 |
BN (mp-984) | <0 0 1> | <0 1 0> | 301.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 251.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 314.6 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 324.6 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 200.7 |
Al (mp-134) | <1 1 0> | <0 1 0> | 301.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 251.7 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 241.4 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 1> | 282.4 |
CdTe (mp-406) | <1 1 0> | <1 0 -1> | 259.6 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 282.4 |
GaSe (mp-1943) | <1 0 1> | <1 1 1> | 213.3 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 1> | 94.1 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 94.1 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 125.8 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 -1> | 259.6 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 100.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 250.9 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 301.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Co5(P2O7)4 (mp-704226) | 0.5937 | 0.113 | 3 |
Mn3(P2O7)2 (mp-706469) | 0.6038 | 0.058 | 3 |
Fe5(P2O7)4 (mp-705433) | 0.6058 | 0.049 | 3 |
Cu2P3O10 (mp-26532) | 0.5401 | 0.038 | 3 |
Mn2P3O10 (mp-31981) | 0.5868 | 0.030 | 3 |
LiCr(PO3)3 (mp-779171) | 0.4598 | 0.042 | 4 |
LiNi(PO3)3 (mp-689961) | 0.4421 | 0.029 | 4 |
LiCuP4O11 (mp-780764) | 0.4764 | 0.083 | 4 |
LiFe(PO3)3 (mp-762657) | 0.5034 | 0.052 | 4 |
Li2Cu(PO3)4 (mp-758929) | 0.4549 | 0.060 | 4 |
Na3LiMg4(Si2O5)6 (mp-695366) | 0.6051 | 0.710 | 5 |
NaCaGaSi2O7 (mp-698690) | 0.5709 | 0.666 | 5 |
Li2CuP3(HO5)2 (mp-849277) | 0.5259 | 0.085 | 5 |
LiAg2P3(HO5)2 (mp-695951) | 0.4271 | 0.020 | 5 |
LiCu2P3(HO5)2 (mp-849424) | 0.6261 | 0.073 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-7.0776 eV |
Corrected Energy-275.0108 eV
-275.0108 eV = -254.7942 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)