Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.095 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.030 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTeO2 + Li2TiTeO6 + Li2TeO4 |
Band Gap1.648 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2 [3] |
HallP 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 210.8 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 342.5 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 259.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 229.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 289.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 263.5 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 198.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 134.0 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 316.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 137.9 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 155.6 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 158.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 223.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 105.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 198.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 312.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 312.7 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 137.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 342.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 259.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 223.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 134.0 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 207.4 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 198.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 44.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 134.0 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 207.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 223.3 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 155.6 |
CdS (mp-672) | <1 0 0> | <1 1 -1> | 269.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 89.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 259.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 264.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 213.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 223.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 223.3 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 259.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 237.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 264.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 247.9 |
YVO4 (mp-19133) | <1 0 0> | <1 1 -1> | 134.7 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 289.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 207.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 237.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 89.3 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 237.1 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 330.7 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 259.3 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 264.6 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 268.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2SiO5 (mp-9515) | 0.4447 | 0.100 | 3 |
ZnSbO3 (mvc-3953) | 0.4332 | 0.161 | 3 |
MgSbO3 (mvc-15602) | 0.4167 | 0.159 | 3 |
MgSbO3 (mvc-13644) | 0.4457 | 0.198 | 3 |
LiTeO3 (mp-755231) | 0.4258 | 0.063 | 3 |
Li4V(TeO4)3 (mp-779999) | 0.2309 | 0.036 | 4 |
Li3Cu(TeO3)4 (mp-761021) | 0.3268 | 0.102 | 4 |
Li4Mn(TeO4)3 (mp-777779) | 0.2696 | 0.045 | 4 |
Li4Fe(TeO4)3 (mp-776188) | 0.2805 | 0.184 | 4 |
Li4Sb(TeO4)3 (mp-776021) | 0.2763 | 0.071 | 4 |
V6O11 (mp-510127) | 0.4774 | 0.013 | 2 |
V7O13 (mp-556332) | 0.4772 | 0.038 | 2 |
V7O13 (mp-623373) | 0.4757 | 0.038 | 2 |
Ti4O7 (mp-558097) | 0.4773 | 0.007 | 2 |
V5O9 (mp-704305) | 0.4485 | 0.008 | 2 |
Li4FeSb(TeO6)2 (mp-780741) | 0.4580 | 3.378 | 5 |
Li4MnSb(WO6)2 (mp-779994) | 0.4439 | 0.041 | 5 |
Li4FeTe2WO12 (mp-775176) | 0.4519 | 0.208 | 5 |
Li4NbFe(TeO6)2 (mp-776914) | 0.4558 | 0.030 | 5 |
Li4FeBi(TeO6)2 (mp-776005) | 0.4252 | 0.036 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ti_pv Te O |
Final Energy/Atom-5.8906 eV |
Corrected Energy-126.0553 eV
Uncorrected energy = -117.8113 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Corrected energy = -126.0553 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)