Final Magnetic Moment15.014 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.607 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.049 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2MnSiO4 + Mn2SiO4 |
Band Gap2.051 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 206.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 325.3 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 137.6 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 206.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 117.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 232.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 139.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 185.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 139.4 |
GaN (mp-804) | <1 1 1> | <0 1 -1> | 277.9 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 283.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 137.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 325.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 234.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 325.3 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 232.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 139.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 325.3 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 161.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 232.3 |
InAs (mp-20305) | <1 1 0> | <1 1 1> | 161.2 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 206.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 325.3 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 161.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 139.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 139.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 325.3 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 206.3 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 232.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 325.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 325.3 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 206.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 325.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 -1 0> | 131.8 |
BN (mp-984) | <0 0 1> | <0 1 1> | 283.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 232.3 |
BN (mp-984) | <1 0 1> | <1 -1 0> | 263.7 |
SiC (mp-7631) | <1 1 0> | <1 1 1> | 161.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 46.5 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 139.4 |
MgO (mp-1265) | <1 1 1> | <0 1 0> | 275.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 137.6 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 275.1 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 1> | 161.2 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 1 0> | 206.3 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 206.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 46.5 |
C (mp-66) | <1 0 0> | <0 0 1> | 232.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 92.9 |
C (mp-66) | <1 1 1> | <0 1 1> | 283.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiAgF3 (mp-752605) | 0.7271 | 0.051 | 3 |
Li2FeF4 (mp-777457) | 0.7223 | 0.054 | 3 |
Li2WO4 (mp-18933) | 0.6968 | 0.005 | 3 |
Li2MnF4 (mp-778731) | 0.7451 | 0.051 | 3 |
Li6Cu5F14 (mp-760015) | 0.7374 | 0.061 | 3 |
LiCoPO4 (mp-863861) | 0.5320 | 0.080 | 4 |
Na2Zn3(SiO4)2 (mp-555300) | 0.3360 | 0.000 | 4 |
Li2Co3(SiO4)2 (mp-763462) | 0.1915 | 0.020 | 4 |
Li2Fe3(SiO4)2 (mp-762716) | 0.2151 | 0.192 | 4 |
Li2Si2Ni3O8 (mp-768050) | 0.2311 | 0.083 | 4 |
Li4TiCu3(PO4)4 (mp-760136) | 0.6463 | 0.090 | 5 |
Li5Co2Cu2(PO4)4 (mp-766608) | 0.6254 | 0.061 | 5 |
SrLi4Ca(SiO4)2 (mp-555089) | 0.6342 | 0.000 | 5 |
Na2TiZn2SiO7 (mp-13810) | 0.6255 | 0.000 | 5 |
Li3Mn2P2(O4F)2 (mp-763234) | 0.6703 | 0.024 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Si O |
Final Energy/Atom-7.3451 eV |
Corrected Energy-362.5127 eV
-362.5127 eV = -330.5301 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 15.1277 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)