Final Magnetic Moment36.962 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.456 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.056 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn2BO4 + LiMnBO3 + Mn3O4 + Li3B7O12 |
Band Gap0.040 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 274.5 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 242.3 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 242.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 339.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 242.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 54.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 274.5 |
GaAs (mp-2534) | <1 1 1> | <0 1 1> | 223.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 145.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 290.8 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 242.4 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 329.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 290.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 145.4 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 223.3 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 223.3 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 274.5 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 242.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 290.8 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 274.5 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 219.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 329.4 |
BN (mp-984) | <0 0 1> | <0 1 1> | 223.3 |
BN (mp-984) | <1 0 0> | <0 1 0> | 329.4 |
BN (mp-984) | <1 0 1> | <1 0 0> | 284.6 |
Al (mp-134) | <1 1 0> | <0 1 0> | 274.5 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 164.7 |
SiC (mp-7631) | <1 1 1> | <0 1 0> | 164.7 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 96.9 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 109.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 339.3 |
C (mp-66) | <1 1 1> | <0 1 0> | 274.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 0> | 219.6 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 1 0> | 109.8 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 109.7 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 274.5 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 274.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 48.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 145.4 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 297.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 242.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 290.8 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 297.7 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 148.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 242.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 274.5 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 274.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 274.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 290.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 339.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3CoO3 (mp-777919) | 0.7425 | 0.127 | 3 |
Li5Fe8(BO3)8 (mp-764891) | 0.2140 | 0.035 | 4 |
Li5Mn8(BO3)8 (mp-777473) | 0.2211 | 0.054 | 4 |
Li5Mn8(BO3)8 (mp-777243) | 0.2130 | 0.053 | 4 |
Li3Mn4(BO3)4 (mp-778867) | 0.1850 | 0.037 | 4 |
Li5Mn8(BO3)8 (mp-778680) | 0.2022 | 0.052 | 4 |
Li4Mn2Fe(BO3)4 (mp-767650) | 0.5073 | 0.075 | 5 |
Li8MnFe7(BO3)8 (mp-850743) | 0.5343 | 0.017 | 5 |
Li4MnFe2(BO3)4 (mp-767642) | 0.4355 | 0.055 | 5 |
Li8Mn5Fe3(BO3)8 (mp-780292) | 0.5395 | 0.011 | 5 |
Li8Mn3Fe5(BO3)8 (mp-775252) | 0.5347 | 0.012 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv B O |
Final Energy/Atom-7.4500 eV |
Corrected Energy-365.0832 eV
Uncorrected energy = -335.2512 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-1.668 eV/atom x 8.0 atoms) = -13.3440 eV
Corrected energy = -365.0832 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)