Final Magnetic Moment5.072 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.188 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.002 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.30 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToKP(HO2)2 + KMn6P7O24 + KP2H5O8 + H2O |
Band Gap4.251 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 173.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 111.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 189.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 111.8 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 189.2 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 173.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 111.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 189.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 266.4 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 189.2 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 266.4 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 189.2 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 152.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 152.6 |
BN (mp-984) | <0 0 1> | <1 0 0> | 152.6 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 152.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 111.8 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 266.4 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 189.2 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 111.8 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 111.8 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 1> | 189.2 |
TbScO3 (mp-31119) | <0 1 1> | <0 1 0> | 266.4 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 111.8 |
Ni (mp-23) | <1 1 0> | <0 1 1> | 173.9 |
InSb (mp-20012) | <1 1 0> | <1 0 1> | 189.2 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 1> | 189.2 |
SiC (mp-11714) | <1 1 0> | <0 1 0> | 266.4 |
MoSe2 (mp-1634) | <1 0 1> | <0 1 0> | 266.4 |
Au (mp-81) | <1 1 0> | <0 1 0> | 266.4 |
NdGaO3 (mp-3196) | <0 1 1> | <0 1 0> | 266.4 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 152.6 |
WSe2 (mp-1821) | <0 0 1> | <1 0 0> | 152.6 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 111.8 |
CaCO3 (mp-3953) | <1 0 0> | <0 1 1> | 173.9 |
TiO2 (mp-390) | <1 1 0> | <0 1 0> | 266.4 |
SrTiO3 (mp-4651) | <1 0 0> | <0 1 0> | 133.2 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 111.8 |
CsI (mp-614603) | <1 1 0> | <0 1 0> | 266.4 |
MgF2 (mp-1249) | <1 1 1> | <0 1 0> | 266.4 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 111.8 |
ZnO (mp-2133) | <1 1 1> | <1 0 1> | 189.2 |
Ge (mp-32) | <1 1 0> | <1 0 1> | 189.2 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 0 1> | 189.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
As3(HO2)5 (mp-27404) | 0.6447 | 0.000 | 3 |
CoP4(H5O8)2 (mp-743783) | 0.6851 | 0.000 | 4 |
AgAs3H2O9 (mp-985701) | 0.5103 | 0.000 | 4 |
NaAs3H2O9 (mp-730154) | 0.5610 | 0.000 | 4 |
MnH6(SO4)4 (mp-25770) | 0.6505 | 0.000 | 4 |
MgH6(SO4)4 (mp-24460) | 0.6771 | 0.000 | 4 |
NaFeP3H7O13 (mp-744775) | 0.5531 | 0.003 | 5 |
K2CoP4(HO2)8 (mp-763754) | 0.2022 | 0.034 | 5 |
K2NiP4(HO2)8 (mp-764404) | 0.4843 | 0.000 | 5 |
Rb2MgP4(HO2)8 (mp-863025) | 0.5620 | 0.000 | 5 |
K2ZnP4(HO2)8 (mp-757470) | 0.4962 | 0.010 | 5 |
K2FePH5(CO5)2 (mp-604118) | 0.7333 | 0.119 | 6 |
K2NaCa2TiSi7HO20 (mp-720410) | 0.6155 | 0.000 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: K_sv Mn_pv P H O |
Final Energy/Atom-6.2268 eV |
Corrected Energy-823.7909 eV
-823.7909 eV = -772.1209 eV (uncorrected energy) - 44.9466 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)