Final Magnetic Moment56.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.436 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.081 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiBO2 + Mn2BO4 + LiMnBO3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <1 0 0> | 316.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 263.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 158.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 263.3 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 263.3 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 189.8 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 263.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 158.0 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 210.7 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 105.3 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 316.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 189.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 158.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 263.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 158.0 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 158.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 263.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 316.0 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 263.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 158.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 182.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 189.8 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 263.3 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 210.7 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 263.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 263.3 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 189.8 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 210.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 210.7 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 263.3 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 210.7 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 316.0 |
LaF3 (mp-905) | <1 1 1> | <1 0 0> | 105.3 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 158.0 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 263.3 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 210.7 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 210.7 |
SiC (mp-11714) | <1 0 0> | <1 0 1> | 189.8 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 263.3 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 158.0 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 182.0 |
Au (mp-81) | <1 1 1> | <1 0 0> | 210.7 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 158.0 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 182.0 |
WS2 (mp-224) | <1 0 1> | <0 0 1> | 182.0 |
C (mp-48) | <1 0 0> | <1 0 0> | 210.7 |
C (mp-48) | <1 1 0> | <1 0 0> | 263.3 |
C (mp-48) | <1 1 1> | <1 0 0> | 263.3 |
ZrO2 (mp-2858) | <0 1 1> | <1 0 0> | 263.3 |
ZrO2 (mp-2858) | <1 0 1> | <1 0 0> | 263.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2Mn3(BO3)3 (mp-780582) | 0.0759 | 0.078 | 4 |
Li2Mn3(BO3)3 (mp-849609) | 0.0662 | 0.076 | 4 |
Li2Mn3(BO3)3 (mp-850179) | 0.0761 | 0.077 | 4 |
Li2Mn3(BO3)3 (mp-778775) | 0.0488 | 0.080 | 4 |
Li2Mn3(BO3)3 (mp-779390) | 0.0945 | 0.077 | 4 |
RbFe5O8 (mp-770482) | 0.7128 | 0.160 | 3 |
Li6B4O9 (mp-768875) | 0.6340 | 0.063 | 3 |
Li4MnF7 (mp-767161) | 0.7211 | 0.051 | 3 |
Li4CuF7 (mp-753130) | 0.7053 | 0.084 | 3 |
Li6B4O9 (mp-1020024) | 0.6626 | 0.000 | 3 |
Li3Mn2Fe(BO3)3 (mp-774378) | 0.7326 | 0.002 | 5 |
Li4MnFe2(BO3)4 (mp-767642) | 0.6608 | 0.048 | 5 |
Li4Mn2Fe(BO3)4 (mp-767650) | 0.6276 | 0.068 | 5 |
Li3CuPCO7 (mp-25460) | 0.7189 | 0.044 | 5 |
Li3ZnPCO7 (mp-772753) | 0.7073 | 0.043 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points32 |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv B O |
Final Energy/Atom-7.4002 eV |
Corrected Energy-548.6661 eV
-548.6661 eV = -503.2134 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 20.1702 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)