Final Magnetic Moment13.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.210 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.060 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnCrO4 + Li24Mn11CrO36 + LiCrO2 + MnCr2O4 |
Band Gap0.010 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 123.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 298.8 |
AlN (mp-661) | <1 1 1> | <0 1 -1> | 144.2 |
CeO2 (mp-20194) | <1 0 0> | <0 1 -1> | 144.2 |
Te2W (mp-22693) | <0 1 1> | <0 1 -1> | 288.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 307.2 |
GaAs (mp-2534) | <1 0 0> | <0 1 -1> | 288.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 184.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 245.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 298.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 -1> | 216.2 |
BN (mp-984) | <1 0 1> | <0 1 -1> | 216.2 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 307.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 -1> | 288.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 -1> | 216.2 |
Al (mp-134) | <1 0 0> | <0 1 -1> | 144.2 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 298.8 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 -1> | 216.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 184.3 |
InAs (mp-20305) | <1 1 0> | <0 1 -1> | 216.2 |
ZnSe (mp-1190) | <1 0 0> | <0 1 -1> | 288.3 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 199.2 |
SiC (mp-7631) | <0 0 1> | <0 1 -1> | 288.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 -1> | 144.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 184.3 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 307.2 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 -1> | 123.3 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 61.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 245.8 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 117.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 199.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 307.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 307.2 |
C (mp-66) | <1 1 1> | <0 1 -1> | 216.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 307.2 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 184.3 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 184.3 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 245.8 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 298.8 |
Ag (mp-124) | <1 0 0> | <0 1 -1> | 288.3 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 99.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 61.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 -1> | 288.3 |
PbS (mp-21276) | <1 0 0> | <0 1 -1> | 72.1 |
PbS (mp-21276) | <1 1 0> | <0 1 1> | 99.8 |
BN (mp-984) | <0 0 1> | <0 1 -1> | 288.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 307.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 245.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 184.3 |
InP (mp-20351) | <1 0 0> | <0 1 -1> | 72.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Mn4O8 (mp-765459) | 0.2255 | 0.058 | 3 |
Li7(NiO2)9 (mp-762007) | 0.1950 | 0.018 | 3 |
Li4Ti3O8 (mp-755266) | 0.2198 | 0.061 | 3 |
Li3Mn4O8 (mp-763710) | 0.2285 | 0.027 | 3 |
Li8V11O22 (mp-768084) | 0.1764 | 0.046 | 3 |
Li3Mn2Cr2O8 (mp-780751) | 0.1831 | 0.062 | 4 |
Li3Mn2(FeO4)2 (mp-767363) | 0.2023 | 0.101 | 4 |
Li3Mn2(CoO4)2 (mp-778583) | 0.1728 | 0.391 | 4 |
Li6MgNi7O16 (mp-769569) | 0.1801 | 0.037 | 4 |
Li3Cr3FeO8 (mp-770226) | 0.1728 | 0.609 | 4 |
Ni6O7 (mp-767815) | 0.2560 | 0.057 | 2 |
Fe9O10 (mp-763441) | 0.2964 | 0.039 | 2 |
Fe7O8 (mp-715333) | 0.2649 | 0.063 | 2 |
Fe8O9 (mp-705588) | 0.2630 | 0.049 | 2 |
Ni6Cl7 (mp-1022720) | 0.2568 | 0.376 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.3861 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Cr_pv O |
Final Energy/Atom-6.8728 eV |
Corrected Energy-464.3911 eV
-464.3911 eV = -412.3671 eV (uncorrected energy) - 29.5508 eV (MP Advanced Correction) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)