Final Magnetic Moment28.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.616 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.077 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeO + FeF2 + LiF |
Band Gap2.401 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 100.3 |
CeO2 (mp-20194) | <1 0 0> | <0 1 -1> | 153.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 167.1 |
GaAs (mp-2534) | <1 0 0> | <0 1 -1> | 307.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 233.9 |
BaF2 (mp-1029) | <1 0 0> | <0 1 -1> | 76.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 233.9 |
GaN (mp-804) | <1 1 1> | <0 1 -1> | 153.7 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 332.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 318.3 |
KCl (mp-23193) | <1 1 0> | <1 1 -1> | 167.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 167.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 -1> | 307.3 |
InAs (mp-20305) | <1 1 0> | <1 -1 0> | 108.7 |
ZnSe (mp-1190) | <1 0 0> | <0 1 -1> | 307.3 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 254.6 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 254.6 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 332.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 66.5 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 332.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 233.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 33.4 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 332.6 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 167.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 33.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 63.8 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 332.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 167.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 233.9 |
Ag (mp-124) | <1 0 0> | <0 1 -1> | 153.7 |
Ag (mp-124) | <1 1 0> | <1 -1 0> | 217.3 |
BaF2 (mp-1029) | <1 1 0> | <1 -1 0> | 108.7 |
GaN (mp-804) | <1 0 0> | <1 -1 0> | 217.3 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 133.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 300.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 266.1 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 199.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 300.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 233.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 300.8 |
InAs (mp-20305) | <1 0 0> | <0 1 -1> | 76.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 233.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 233.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 233.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 133.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 100.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 300.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 133.7 |
Te2W (mp-22693) | <1 0 1> | <1 1 0> | 199.6 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 133.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn(FeO2)2 (mp-743547) | 0.1295 | 0.503 | 3 |
Mg(NiO2)2 (mvc-5456) | 0.1264 | 0.118 | 3 |
Mg(CuO2)2 (mvc-4858) | 0.1270 | 0.090 | 3 |
Zn(CuO2)2 (mvc-4855) | 0.1204 | 0.019 | 3 |
Li(Fe2O3)4 (mp-997515) | 0.1011 | 0.052 | 3 |
Li5Mn2Fe17O32 (mp-777733) | 0.1207 | 0.065 | 4 |
Li3Mg2Fe19O32 (mp-771996) | 0.1261 | 0.070 | 4 |
LiZn2Fe9O16 (mp-771993) | 0.1314 | 0.069 | 4 |
Li3Zn(Fe5O8)4 (mp-771780) | 0.1029 | 0.068 | 4 |
Li5Co7O3F13 (mp-849472) | 0.0965 | 0.053 | 4 |
Fe3O4 (mp-715491) | 0.2109 | 0.017 | 2 |
Fe3O4 (mp-542433) | 0.2062 | 0.075 | 2 |
Fe3O4 (mp-650112) | 0.1843 | 0.060 | 2 |
Fe3O4 (mp-715558) | 0.2137 | 0.785 | 2 |
Fe3O4 (mp-715811) | 0.2169 | 0.037 | 2 |
Li4Ti3Cr3(SnO8)2 (mp-776780) | 0.1948 | 0.138 | 5 |
Li4Fe3Cu3(SbO8)2 (mp-764385) | 0.2004 | 0.031 | 5 |
Li4Cr3Ni3(TeO8)2 (mp-761407) | 0.1974 | 0.179 | 5 |
Li4Ti3Cr3(WO8)2 (mp-773537) | 0.1951 | 0.046 | 5 |
Li4Nb3V3(SnO8)2 (mp-767976) | 0.1780 | 0.129 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.7024 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6876 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6952 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6994 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7001 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv O F |
Final Energy/Atom-5.5058 eV |
Corrected Energy-175.4010 eV
-175.4010 eV = -154.1632 eV (uncorrected energy) - 19.1310 eV (MP Advanced Correction) - 2.1069 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)