Final Magnetic Moment9.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.303 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.084 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoO + CoF2 + LiF |
Band Gap2.008 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 201.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 269.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 134.1 |
GaAs (mp-2534) | <1 1 1> | <1 -1 -1> | 285.9 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 268.3 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 268.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 201.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 268.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 -1 -1> | 285.9 |
InAs (mp-20305) | <1 0 0> | <1 -1 -1> | 190.6 |
AlN (mp-661) | <1 0 1> | <0 1 -1> | 271.6 |
BaF2 (mp-1029) | <1 0 0> | <1 -1 -1> | 190.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 134.1 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 232.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 -1> | 271.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 -1> | 135.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 134.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 134.1 |
ZnSe (mp-1190) | <1 1 1> | <1 -1 -1> | 285.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 -1 -1> | 285.9 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 115.6 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 201.2 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 202.5 |
YVO4 (mp-19133) | <1 0 1> | <1 -1 -1> | 285.9 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 201.2 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 163.6 |
BN (mp-984) | <1 0 1> | <0 1 0> | 201.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 163.6 |
Al (mp-134) | <1 1 1> | <1 0 0> | 202.5 |
SiC (mp-7631) | <0 0 1> | <0 1 -1> | 271.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 231.3 |
Fe3O4 (mp-19306) | <1 1 0> | <0 1 0> | 201.2 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 201.2 |
TeO2 (mp-2125) | <0 1 1> | <0 1 1> | 231.3 |
TeO2 (mp-2125) | <1 0 1> | <0 1 1> | 231.3 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 -1> | 135.8 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 0> | 268.3 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 134.1 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 163.6 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 272.2 |
TiO2 (mp-2657) | <0 0 1> | <1 1 -1> | 191.6 |
TiO2 (mp-2657) | <1 0 1> | <0 1 1> | 231.3 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 201.2 |
GdScO3 (mp-5690) | <1 0 1> | <1 -1 -1> | 285.9 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 268.3 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 268.3 |
GaP (mp-2490) | <1 1 0> | <0 1 0> | 134.1 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 201.2 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 -1> | 135.8 |
TbScO3 (mp-31119) | <0 1 1> | <0 1 0> | 268.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sn2N2O (mp-762347) | 0.3620 | 0.064 | 3 |
Mn3Fe5O12 (mp-761939) | 0.3626 | 0.076 | 3 |
Mn2OF2 (mp-764411) | 0.2177 | 0.066 | 3 |
Sn2N2O (mp-773830) | 0.2610 | 0.063 | 3 |
Sn2N2O (mp-776966) | 0.2853 | 0.061 | 3 |
LiMn3OF5 (mp-764307) | 0.3840 | 0.069 | 4 |
LiMn7(OF3)3 (mp-764403) | 0.3948 | 0.060 | 4 |
Li3Co13O5F19 (mp-764094) | 0.3365 | 0.090 | 4 |
LiCo3OF5 (mp-850139) | 0.3920 | 0.091 | 4 |
LiFe3OF5 (mp-764579) | 0.4090 | 0.086 | 4 |
Fe2O3 (mp-777192) | 0.5339 | 0.732 | 2 |
Fe2O3 (mp-715572) | 0.5537 | 0.116 | 2 |
P4Ru (mp-27173) | 0.6171 | 0.000 | 2 |
Fe2O3 (mp-715276) | 0.6184 | 0.086 | 2 |
Mn2O3 (mp-565203) | 0.5954 | 0.000 | 2 |
Li4Nb3Cu3(SnO8)2 (mp-775145) | 0.4493 | 0.125 | 5 |
Li4Cu3Ni3(WO8)2 (mp-773508) | 0.4943 | 0.038 | 5 |
Li4Ti3Mn3(WO8)2 (mp-772490) | 0.4584 | 0.060 | 5 |
Li4Ti3Mn3Nb2O16 (mp-776061) | 0.4993 | 0.042 | 5 |
Li4Ti3Nb2Fe3O16 (mp-775999) | 0.4828 | 0.018 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co O F |
Final Energy/Atom-5.1994 eV |
Corrected Energy-233.2751 eV
-233.2751 eV = -207.9780 eV (uncorrected energy) - 22.4880 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)