Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.558 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.068 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.86 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Si2O5 + Fe2O3 |
Band Gap2.730 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPna21 [33] |
HallP 2c 2n |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 205.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 223.2 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 222.5 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 137.2 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 201.0 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 205.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 90.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 286.9 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 68.6 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 274.4 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 95.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 255.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 127.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 286.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 67.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 350.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 222.5 |
Te2W (mp-22693) | <0 1 1> | <1 1 1> | 287.6 |
Te2W (mp-22693) | <1 0 1> | <0 1 1> | 205.8 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 286.9 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 180.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 350.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 223.2 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 74.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 318.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 191.3 |
BN (mp-984) | <1 0 1> | <1 1 0> | 180.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 95.6 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 223.2 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 159.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 318.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 286.9 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 303.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 127.5 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 121.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 286.9 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 223.2 |
Al (mp-134) | <1 1 0> | <1 1 0> | 90.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 222.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 134.0 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 60.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 137.2 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 180.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 286.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 137.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 68.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 182.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 60.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 159.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 90.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn2SiO4 (mp-3789) | 0.4828 | 0.000 | 3 |
Be(GaO2)2 (mp-676950) | 0.4584 | 0.116 | 3 |
Zn2SiO4 (mp-1020636) | 0.5017 | 0.052 | 3 |
Li2BeF4 (mp-4622) | 0.4851 | 0.000 | 3 |
Li2SeO4 (mp-4855) | 0.4989 | 0.000 | 3 |
LiFeSiO4 (mp-863887) | 0.3434 | 0.352 | 4 |
LiFeSiO4 (mp-767838) | 0.2602 | 0.070 | 4 |
LiFeSiO4 (mp-997531) | 0.3116 | 0.732 | 4 |
LiCoSiO4 (mp-779192) | 0.3076 | 0.353 | 4 |
LiFeSiO4 (mp-762703) | 0.3367 | 0.376 | 4 |
CuS2 (mp-684604) | 0.7125 | 0.100 | 2 |
BN (mp-1077506) | 0.6900 | 0.302 | 2 |
SiC2 (mp-1019097) | 0.6529 | 0.562 | 2 |
CN2 (mp-1077595) | 0.6332 | 0.691 | 2 |
Ti3N4 (mp-1080190) | 0.7003 | 0.119 | 2 |
Be3Fe4Si3SO12 (mp-627398) | 0.4862 | 0.203 | 5 |
Li4Ga3Si3IO12 (mp-557112) | 0.5144 | 0.000 | 5 |
Mn4Be3Ge3SeO12 (mp-25766) | 0.5294 | 0.000 | 5 |
Mn4Be3Ge3SO12 (mp-25772) | 0.5222 | 0.000 | 5 |
Be3Fe4Si3TeO12 (mp-704630) | 0.5229 | 0.168 | 5 |
Na2Li2Al3Si3ClO12 (mp-43030) | 0.4972 | 0.003 | 6 |
C (mp-568410) | 0.6310 | 0.507 | 1 |
C (mp-1008374) | 0.6476 | 0.437 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Si O |
Final Energy/Atom-6.8512 eV |
Corrected Energy-214.0025 eV
-214.0025 eV = -191.8338 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)