Final Magnetic Moment33.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.082 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.111 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCo3O4 + CoO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4 [82] |
HallI 4 |
Point Group4 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 203.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 161.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 161.2 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 190.6 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 190.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 161.2 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 190.6 |
LaF3 (mp-905) | <1 1 0> | <1 0 1> | 190.6 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 190.6 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 1> | 190.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 161.2 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 101.6 |
C (mp-48) | <1 1 0> | <1 0 0> | 101.6 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 161.2 |
SrTiO3 (mp-4651) | <1 1 1> | <1 1 0> | 143.7 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 161.2 |
LiAlO2 (mp-3427) | <1 1 0> | <1 0 1> | 190.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMn28O56 (mp-775739) | 0.1402 | 0.033 | 3 |
LiMn12O24 (mp-694894) | 0.1626 | 0.044 | 3 |
Mn9(FeO6)4 (mp-769622) | 0.2975 | 0.081 | 3 |
LiMn10O20 (mp-768056) | 0.2127 | 0.034 | 3 |
LiMn8O16 (mp-705612) | 0.2635 | 0.032 | 3 |
Li3Mn5Cr3O16 (mp-775496) | 0.7378 | 0.005 | 4 |
Li2Fe3O3F5 (mp-849525) | 0.6363 | 0.102 | 4 |
LiMn3CrO8 (mp-773299) | 0.5213 | 0.112 | 4 |
Co2S3 (mp-684732) | 0.7226 | 0.026 | 2 |
Mn21O40 (mp-767941) | 0.1435 | 0.053 | 2 |
Co5O8 (mp-761471) | 0.5337 | 0.042 | 2 |
Fe5O8 (mp-543082) | 0.7128 | 0.163 | 2 |
Mn21O40 (mp-849596) | 0.2324 | 0.044 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Co O |
Final Energy/Atom-5.6684 eV |
Corrected Energy-413.2173 eV
-413.2173 eV = -345.7717 eV (uncorrected energy) - 39.3540 eV (MP Advanced Correction) - 28.0916 eV (MP Anion Correction)
|