Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.782 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.037 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCoO2 |
Band Gap1.872 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 238.4 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 202.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 201.9 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 287.4 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 190.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 269.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 33.7 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 47.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 168.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 302.9 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 116.7 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 333.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 201.9 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 151.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 175.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 226.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 143.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 168.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 95.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 134.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 226.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 233.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 168.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 302.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 302.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 33.7 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 47.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 168.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 33.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 47.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 58.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 235.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 168.3 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 238.4 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 269.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 33.7 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 47.7 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 58.4 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 286.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 269.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 168.3 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 190.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 33.7 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 47.7 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 58.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 117.1 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 175.1 |
BN (mp-984) | <0 0 1> | <0 1 1> | 175.1 |
BN (mp-984) | <1 0 1> | <1 1 1> | 226.5 |
BN (mp-984) | <1 1 0> | <0 1 0> | 333.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5Fe7O12 (mp-771531) | 0.1462 | 0.025 | 3 |
Li7Ti5O12 (mp-779455) | 0.1656 | 0.014 | 3 |
Li5V7O12 (mp-764746) | 0.1304 | 0.369 | 3 |
Li5Fe11O16 (mp-762692) | 0.1345 | 0.043 | 3 |
LiCoO2 (mp-1097885) | 0.1108 | 0.043 | 3 |
Li4AlCr3O8 (mp-771377) | 0.1187 | 0.031 | 4 |
Li4AlCr3O8 (mp-770240) | 0.1203 | 0.204 | 4 |
Li4Cr3CoO8 (mp-770234) | 0.1199 | 0.255 | 4 |
Li4Cr3NiO8 (mp-770046) | 0.1155 | 0.017 | 4 |
Li5Fe5(SbO6)2 (mp-771103) | 0.1165 | 0.055 | 4 |
LiTe3 (mp-27466) | 0.2660 | 0.009 | 2 |
Bi2Te3 (mp-568390) | 0.2946 | 0.248 | 2 |
In2Se3 (mp-1068548) | 0.3006 | 0.530 | 2 |
In2Se3 (mp-20830) | 0.2853 | 0.530 | 2 |
Sb2Te3 (mp-1080789) | 0.3099 | 0.129 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.5207 | 0.005 | 5 |
Hg (mp-982872) | 0.4581 | 0.020 | 1 |
Sb (mp-632286) | 0.4115 | 0.059 | 1 |
Te (mp-570459) | 0.4604 | 0.044 | 1 |
Te (mp-10654) | 0.4846 | 0.047 | 1 |
Te (mp-105) | 0.4014 | 0.047 | 1 |
Explore more synthesis descriptions for materials of composition LiCoO2.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co O |
Final Energy/Atom-5.6903 eV |
Corrected Energy-104.1585 eV
-104.1585 eV = -91.0441 eV (uncorrected energy) - 7.4960 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)