Final Magnetic Moment14.997 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.890 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.071 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnO + LiF + MnF2 |
Band Gap1.775 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 326.3 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 326.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 139.8 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 201.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 266.9 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 201.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 326.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 314.4 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 251.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 177.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 139.8 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 201.4 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 326.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 326.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 251.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 279.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 266.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 326.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 326.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 207.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 314.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 326.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 266.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 326.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 237.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 201.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 251.8 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 251.8 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 285.5 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 203.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 326.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 207.6 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 251.8 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 302.2 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 326.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 118.6 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 279.5 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 279.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 296.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 177.9 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 209.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 203.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 148.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 237.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 148.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 266.9 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 244.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 296.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 349.4 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 326.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4Mn3O8 (mp-780711) | 0.5242 | 0.028 | 3 |
Ca2Tl2O5 (mp-861057) | 0.4270 | 0.001 | 3 |
Ca3Tl4O9 (mp-765585) | 0.4015 | 0.005 | 3 |
Sr2Tl2O5 (mp-757407) | 0.4875 | 0.000 | 3 |
Mg2Co9O13 (mvc-2285) | 0.5079 | 0.145 | 3 |
Li4Mn5O9F (mp-767113) | 0.5358 | 0.061 | 4 |
Li3Fe2Ni3O10 (mp-762777) | 0.4852 | 0.098 | 4 |
Li2Fe2OF4 (mp-764564) | 0.4870 | 0.085 | 4 |
Li2Mn(CoO3)2 (mp-778337) | 0.5053 | 0.097 | 4 |
Li4Mn3O5F3 (mp-767143) | 0.5368 | 0.096 | 4 |
Cr3N4 (mp-1014365) | 0.5567 | 0.200 | 2 |
Fe15O16 (mp-705551) | 0.5262 | 0.060 | 2 |
Fe3O4 (mp-715438) | 0.5083 | 0.062 | 2 |
Ni15O16 (mp-691155) | 0.6420 | 0.103 | 2 |
Ni15O16 (mp-33255) | 0.6444 | 0.103 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv O F |
Final Energy/Atom-5.7442 eV |
Corrected Energy-97.6528 eV
-97.6528 eV = -91.9080 eV (uncorrected energy) - 5.0426 eV (MP Advanced Correction) - 0.7023 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)