Final Magnetic Moment10.012 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.656 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.031 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnPO4 + Li3PO4 |
Band Gap3.918 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 77.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 111.9 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 134.6 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 111.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 310.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 77.6 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 111.9 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 134.6 |
Ag (mp-124) | <1 0 0> | <1 1 -1> | 156.9 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 223.9 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 223.9 |
BN (mp-984) | <1 1 0> | <0 1 1> | 134.6 |
BN (mp-984) | <1 1 1> | <0 1 1> | 134.6 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 189.7 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 219.9 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 155.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 1> | 189.7 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 219.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 310.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 232.9 |
C (mp-66) | <1 1 1> | <0 1 1> | 134.6 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 310.5 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 155.2 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 310.5 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 310.5 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 310.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 155.2 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 77.6 |
PbSe (mp-2201) | <1 1 0> | <1 0 -1> | 111.9 |
PbSe (mp-2201) | <1 1 1> | <0 1 1> | 134.6 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 232.9 |
CaCO3 (mp-3953) | <1 1 0> | <0 0 1> | 155.2 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 232.9 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 1 -1> | 156.9 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 77.6 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 155.2 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 310.5 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 310.5 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 1> | 134.6 |
Ga2O3 (mp-886) | <1 0 -1> | <1 1 -1> | 156.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 310.5 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 -1> | 223.9 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 77.6 |
GaSb (mp-1156) | <1 1 1> | <0 1 1> | 134.6 |
SrTiO3 (mp-4651) | <0 0 1> | <1 1 -1> | 156.9 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 310.5 |
GaTe (mp-542812) | <0 0 1> | <1 0 -1> | 223.9 |
Au (mp-81) | <1 0 0> | <1 1 -1> | 156.9 |
Au (mp-81) | <1 1 0> | <1 0 -1> | 223.9 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 77.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2PO5 (mp-771449) | 0.6530 | 1.293 | 3 |
Fe4P2O9 (mp-637226) | 0.6027 | 0.391 | 3 |
Mn4P2O9 (mp-770499) | 0.6206 | 0.015 | 3 |
Ni4P2O9 (mp-771899) | 0.6113 | 0.037 | 3 |
MgSiO3 (mp-657336) | 0.5413 | 0.306 | 3 |
Li5Ni2(PO4)3 (mp-777968) | 0.2894 | 0.039 | 4 |
Li4Mn2V3O12 (mp-765660) | 0.4875 | 0.323 | 4 |
Li5Co2(PO4)3 (mp-780435) | 0.2577 | 0.175 | 4 |
LiVSiO4 (mp-767472) | 0.4928 | 0.063 | 4 |
Li5Mn2(PO4)3 (mp-778881) | 0.4539 | 0.284 | 4 |
Li5Mn3Cr(PO4)4 (mp-764909) | 0.5524 | 0.091 | 5 |
Li5Co2Cu2(PO4)4 (mp-766608) | 0.4962 | 0.061 | 5 |
Li4Cu3Sn(PO4)4 (mp-849752) | 0.5912 | 0.077 | 5 |
Na2TiZn2SiO7 (mp-13810) | 0.5479 | 0.000 | 5 |
Li3Mn2P2(O4F)2 (mp-763234) | 0.5198 | 0.024 | 5 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.6835 | 0.008 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-6.8241 eV |
Corrected Energy-647.6732 eV
-647.6732 eV = -600.5165 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 13.4468 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)