Material Details

Final Magnetic Moment
1.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.552 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.091 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.38 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
LiMnPO4
Band Gap
3.524 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.003 340.4
AlN (mp-661) <1 1 1> <0 0 1> 0.011 170.2
YAlO3 (mp-3792) <1 0 1> <0 1 0> 0.016 48.9
Te2W (mp-22693) <0 0 1> <1 0 1> 0.016 66.5
Al (mp-134) <1 0 0> <0 0 1> 0.018 340.4
C (mp-48) <1 0 1> <1 0 1> 0.019 199.5
AlN (mp-661) <1 1 0> <0 0 1> 0.019 136.2
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.024 170.2
SiC (mp-11714) <1 1 0> <0 0 1> 0.029 272.3
KCl (mp-23193) <1 1 1> <1 0 0> 0.029 285.7
LiAlO2 (mp-3427) <1 0 0> <1 0 1> 0.031 66.5
AlN (mp-661) <0 0 1> <0 0 1> 0.032 34.0
LaF3 (mp-905) <0 0 1> <0 0 1> 0.032 136.2
InSb (mp-20012) <1 1 1> <0 0 1> 0.035 306.4
BN (mp-984) <0 0 1> <0 0 1> 0.038 136.2
CdTe (mp-406) <1 1 1> <0 0 1> 0.039 306.4
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.041 102.1
TiO2 (mp-390) <1 0 0> <1 0 1> 0.042 332.5
AlN (mp-661) <1 0 1> <1 0 0> 0.044 285.7
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.047 136.2
BaF2 (mp-1029) <1 0 0> <1 0 1> 0.047 199.5
TiO2 (mp-390) <1 0 1> <1 0 1> 0.048 199.5
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.058 340.4
GaN (mp-804) <0 0 1> <0 1 1> 0.060 178.7
CsI (mp-614603) <1 0 0> <1 1 1> 0.061 247.6
SrTiO3 (mp-4651) <0 0 1> <1 1 1> 0.062 247.6
GaTe (mp-542812) <1 1 0> <0 1 0> 0.065 195.5
LiAlO2 (mp-3427) <0 0 1> <1 0 1> 0.067 332.5
SrTiO3 (mp-4651) <1 1 0> <1 1 1> 0.068 247.6
Ni (mp-23) <1 0 0> <1 1 1> 0.071 247.6
MgO (mp-1265) <1 1 0> <1 0 0> 0.073 228.5
TiO2 (mp-390) <0 0 1> <0 1 0> 0.076 146.7
CdWO4 (mp-19387) <0 1 0> <0 1 1> 0.081 238.3
GaTe (mp-542812) <0 0 1> <1 0 0> 0.082 228.5
CdTe (mp-406) <1 1 0> <0 0 1> 0.091 306.4
LiAlO2 (mp-3427) <1 0 1> <1 1 0> 0.094 300.8
WSe2 (mp-1821) <1 0 0> <1 1 1> 0.097 247.6
YAlO3 (mp-3792) <1 0 0> <0 1 1> 0.097 119.1
KCl (mp-23193) <1 1 0> <1 0 0> 0.100 57.1
NdGaO3 (mp-3196) <1 1 0> <1 1 1> 0.101 247.6
InSb (mp-20012) <1 1 0> <0 0 1> 0.106 306.4
CdS (mp-672) <0 0 1> <0 0 1> 0.109 136.2
CeO2 (mp-20194) <1 0 0> <0 1 1> 0.120 59.6
Si (mp-149) <1 0 0> <0 1 1> 0.122 59.6
Ni (mp-23) <1 1 0> <1 1 1> 0.125 247.6
NdGaO3 (mp-3196) <0 1 0> <0 0 1> 0.126 170.2
WS2 (mp-224) <0 0 1> <0 1 1> 0.135 178.7
MoS2 (mp-1434) <0 0 1> <0 1 1> 0.135 178.7
LiF (mp-1138) <1 1 0> <0 0 1> 0.137 238.3
YAlO3 (mp-3792) <1 1 0> <1 1 1> 0.145 165.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Tl3SbS4 (mp-8378) 0.5699 0.000 3
Li8B2O7 (mp-768921) 0.5815 0.045 3
Rb5FeO4 (mp-770716) 0.5789 0.048 3
Ag2PS3 (mp-561822) 0.4880 0.011 3
Ag2PSe3 (mp-13956) 0.5828 0.000 3
Li3Fe(PO4)2 (mp-761555) 0.5481 0.452 4
LiMnPO4 (mp-861491) 0.4635 0.070 4
RbNa11(WN3)4 (mp-569098) 0.5387 0.006 4
CrHg3(SO2)2 (mp-565438) 0.5233 0.346 4
Na3Sb(PO4)2 (mp-776965) 0.5502 0.011 4
Ga2I3 (mp-636675) 0.7391 0.000 2
K2LiVPO6 (mp-764301) 0.5479 0.080 5
Sr2AlCu2NiO7 (mvc-864) 0.7021 0.141 5
SrZnP2WO8 (mvc-3145) 0.6786 0.279 5
KNaLi2(SO4)2 (mp-14484) 0.6386 0.000 5
Na2TeHSO5F3 (mp-696485) 0.7333 0.016 6
Na2LiCaVP2O9 (mp-763838) 0.7426 0.111 6
NaCaBeSi2O6F (mp-560721) 0.7365 0.000 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

The LiMnPO4 samples were synthesized via a simple solid-state method using lithium carbonate (Li2CO3, Sinopharm, AR), manganese acetate (Mn(CH3COO)2.4H2O, Sinopharm, AR), and ammonium dihydrogen phosp [...]
We prepared LiMnPO4 powders by an ultrasonic spray pyrolysis method. Stoichiometric amounts of lithium dihydrogen phosphate acid (LiH2PO4, Sigma) and manganese nitrate tetrahydrate [Mn(NO3)24H2O, Sig [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition LiMnPO4.

Text computed by synthesisproject.org.

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Mn: 3.9 eV
Pseudopotentials
VASP PAW: Li_sv Mn_pv P O
Final Energy/Atom
-7.0946 eV
Corrected Energy
-216.3118 eV
Uncorrected energy = -198.6478 eV Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV Composition-based energy adjustment (-1.668 eV/atom x 4.0 atoms) = -6.6720 eV Corrected energy = -216.3118 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)