Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.039 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.042 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToWO3 + In2O3 |
Band Gap2.512 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/c [13] |
Hall-P 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 1> | 234.6 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 137.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 231.3 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 68.6 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 231.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 155.9 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 308.6 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 117.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 155.9 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 231.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 155.9 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 185.1 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 246.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 272.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 155.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 272.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 155.9 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 154.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 272.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 350.8 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 272.8 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 272.8 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 193.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 311.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 350.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 -1> | 205.9 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 234.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 265.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 116.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 311.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 246.9 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 155.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 350.8 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 234.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 246.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 272.8 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 289.9 |
BN (mp-984) | <0 0 1> | <1 0 0> | 185.1 |
BN (mp-984) | <1 0 1> | <0 0 1> | 311.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 194.9 |
BN (mp-984) | <1 1 1> | <0 0 1> | 350.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 185.1 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 308.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 272.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 350.8 |
Al (mp-134) | <1 0 0> | <1 0 0> | 246.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 116.9 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 -1> | 68.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 1> | 308.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 350.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TmTaO4 (mp-756898) | 0.5830 | 0.017 | 3 |
MgVF4 (mvc-3716) | 0.5609 | 0.097 | 3 |
Zr5Ti7O24 (mp-860957) | 0.5988 | 0.040 | 3 |
TbTaO4 (mp-756076) | 0.5834 | 0.019 | 3 |
Sr2CaI6 (mp-768734) | 0.5896 | 0.067 | 3 |
LiV2O5F (mp-766776) | 0.5876 | 0.047 | 4 |
YNb2NO5 (mp-776408) | 0.5866 | 0.072 | 4 |
YNb2NO5 (mp-776359) | 0.5426 | 0.064 | 4 |
YCu(WO4)2 (mvc-16327) | 0.5878 | 0.033 | 4 |
YCr(WO4)2 (mvc-608) | 0.5780 | 0.109 | 4 |
BiO2 (mp-557993) | 0.6153 | 0.000 | 2 |
LaMgCrNiO6 (mvc-9871) | 0.7250 | 0.423 | 5 |
LaMgCrAgO6 (mvc-9872) | 0.7143 | 0.225 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: In_d W_pv O |
Final Energy/Atom-6.4376 eV |
Corrected Energy-265.9954 eV
Uncorrected energy = -231.7554 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-4.438 eV/atom x 4.0 atoms) = -17.7520 eV
Corrected energy = -265.9954 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)