material

LiMnPd2

ID:

mp-861629

DOI:

10.17188/1309234


Material Details

Final Magnetic Moment
4.475 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.363 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.91 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <0 0 1> <1 0 0> 0.002 188.0
LiF (mp-1138) <1 0 0> <1 0 0> 0.002 150.4
LiF (mp-1138) <1 1 0> <1 1 0> 0.003 212.7
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.003 260.5
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.007 263.2
SiO2 (mp-6930) <1 1 1> <1 0 0> 0.008 263.2
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.008 225.6
WSe2 (mp-1821) <1 1 0> <1 1 1> 0.008 260.5
Cu (mp-30) <1 0 0> <1 0 0> 0.012 338.4
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.017 65.1
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.017 319.0
Si (mp-149) <1 0 0> <1 0 0> 0.017 150.4
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.019 212.7
Mg (mp-153) <1 1 0> <1 1 0> 0.020 319.0
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.020 150.4
SiC (mp-11714) <1 0 0> <1 0 0> 0.020 188.0
Ge (mp-32) <1 0 0> <1 0 0> 0.021 300.8
SiC (mp-7631) <1 0 0> <1 0 0> 0.022 188.0
Te2Mo (mp-602) <1 1 0> <1 0 0> 0.022 188.0
Mg (mp-153) <1 1 1> <1 0 0> 0.022 150.4
GaN (mp-804) <1 1 0> <1 1 0> 0.024 319.0
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.024 260.5
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.025 260.5
ZnO (mp-2133) <0 0 1> <1 1 1> 0.029 65.1
BN (mp-984) <0 0 1> <1 1 1> 0.032 65.1
GaP (mp-2490) <1 0 0> <1 0 0> 0.033 150.4
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 1 0> 0.037 159.5
Ge3(BiO3)4 (mp-23560) <1 1 1> <1 1 1> 0.038 195.4
SiC (mp-11714) <0 0 1> <1 0 0> 0.040 263.2
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.041 195.4
ZrO2 (mp-2858) <0 1 1> <1 1 1> 0.042 195.4
SiC (mp-7631) <0 0 1> <1 0 0> 0.045 263.2
AlN (mp-661) <0 0 1> <1 1 1> 0.046 260.5
CaCO3 (mp-3953) <1 0 0> <1 1 1> 0.051 260.5
GaN (mp-804) <1 0 1> <1 1 0> 0.054 265.9
WSe2 (mp-1821) <1 1 1> <1 1 1> 0.055 260.5
SiC (mp-8062) <1 1 1> <1 0 0> 0.058 263.2
GaAs (mp-2534) <1 0 0> <1 0 0> 0.060 300.8
CaCO3 (mp-3953) <1 1 0> <1 0 0> 0.064 150.4
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.070 150.4
C (mp-66) <1 0 0> <1 1 0> 0.080 265.9
LiGaO2 (mp-5854) <1 1 0> <1 1 1> 0.089 195.4
Te2Mo (mp-602) <1 1 1> <1 0 0> 0.091 188.0
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.091 195.4
Al (mp-134) <1 1 1> <1 1 1> 0.091 195.4
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.094 300.8
MgO (mp-1265) <1 1 1> <1 0 0> 0.094 188.0
AlN (mp-661) <1 0 0> <1 0 0> 0.096 188.0
Cu (mp-30) <1 1 0> <1 1 0> 0.121 319.0
GaN (mp-804) <1 0 0> <1 0 0> 0.122 188.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
131 103 103 0 0 0
103 131 103 0 0 0
103 103 131 0 0 0
0 0 0 60 0 0
0 0 0 0 60 0
0 0 0 0 0 60
Compliance Tensor Sij (10-12Pa-1)
25.3 -11.2 -11.2 0 0 0
-11.2 25.3 -11.2 0 0 0
-11.2 -11.2 25.3 0 0 0
0 0 0 16.6 0 0
0 0 0 0 16.6 0
0 0 0 0 0 16.6
Shear Modulus GV
42 GPa
Bulk Modulus KV
112 GPa
Shear Modulus GR
26 GPa
Bulk Modulus KR
112 GPa
Shear Modulus GVRH
34 GPa
Bulk Modulus KVRH
112 GPa
Elastic Anisotropy
3.16
Poisson's Ratio
0.36

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
AlVFeCo (mp-1008530) 0.0000 0.027 4
TiFeCoSb (mp-998973) 0.0000 0.198 4
TiAlFeCo (mp-998980) 0.0000 0.000 4
TiFeCoGe (mp-1018012) 0.0000 0.026 4
MnFeCoGe (mp-1018024) 0.0000 0.009 4
CeAg (mp-2756) 0.0000 0.090 2
GdIn (mp-21005) 0.0000 0.000 2
CaPd (mp-213) 0.0000 0.000 2
BeCu (mp-2323) 0.0000 0.011 2
PuBi (mp-1002230) 0.0000 0.000 2
DyMgTl2 (mp-866007) 0.0000 0.000 3
V2CuBr (mp-631442) 0.0000 0.970 3
MgZnPd2 (mp-864923) 0.0000 0.000 3
YDyRh2 (mp-979917) 0.0000 0.009 3
Sc2MnSn (mp-999207) 0.0000 0.314 3
Kr (mp-974400) 0.0000 0.002 1
Ge (mp-998883) 0.0000 0.346 1
Ni (mp-1008728) 0.0000 0.098 1
Si (mp-1014212) 0.0000 0.541 1
Cu (mp-998890) 0.0000 0.035 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Mn_pv Pd
Final Energy/Atom
-5.7214 eV
Corrected Energy
-22.8854 eV
-22.8854 eV = -22.8854 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)