Final Magnetic Moment-0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.538 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.006 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAcAu3 + AcZn3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 0> | 303.0 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 227.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 267.8 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 278.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 267.8 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 227.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 267.8 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 227.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 214.2 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 151.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 214.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 267.8 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 227.2 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 278.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 227.2 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 151.5 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 227.2 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 227.2 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 227.2 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 267.8 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 214.2 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 227.2 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 278.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 267.8 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 278.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 267.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 278.3 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 267.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 92.8 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 227.2 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 227.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 53.6 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 214.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 321.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 214.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 267.8 |
Al (mp-134) | <1 0 0> | <1 0 0> | 214.2 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 267.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 321.4 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 92.8 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 75.7 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 92.8 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 107.1 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 321.4 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 227.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 267.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 267.8 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 214.2 |
C (mp-66) | <1 0 0> | <1 0 0> | 214.2 |
C (mp-66) | <1 1 0> | <1 1 0> | 303.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlVFeCo (mp-1008530) | 0.0000 | 0.028 | 4 |
TiFeCoSb (mp-998973) | 0.0000 | 0.198 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.025 | 4 |
MnFeCoGe (mp-1018024) | 0.0000 | 0.009 | 4 |
CeAg (mp-2756) | 0.0000 | 0.028 | 2 |
GdIn (mp-21005) | 0.0000 | 0.000 | 2 |
CaPd (mp-213) | 0.0000 | 0.000 | 2 |
BeCu (mp-2323) | 0.0000 | 0.012 | 2 |
PuBi (mp-1002230) | 0.0000 | 0.015 | 2 |
Ba2HgPb (mp-866106) | 0.0000 | 0.000 | 3 |
YbHgPd2 (mp-865766) | 0.0000 | 0.000 | 3 |
Be2PdRh (mp-866115) | 0.0000 | 0.000 | 3 |
Ca2AgPb (mp-864991) | 0.0000 | 0.000 | 3 |
Ac2ZnSi (mp-866289) | 0.0000 | 0.000 | 3 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
Ge (mp-998883) | 0.0000 | 0.346 | 1 |
Ni (mp-1008728) | 0.0000 | 0.097 | 1 |
Si (mp-1014212) | 0.0000 | 0.541 | 1 |
Cu (mp-998890) | 0.0000 | 0.034 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points28 |
U Values-- |
PseudopotentialsVASP PAW: Ac Zn Au |
Final Energy/Atom-3.5192 eV |
Corrected Energy-14.0768 eV
-14.0768 eV = -14.0768 eV (uncorrected energy)
|