Final Magnetic Moment0.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.399 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.26 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 119.8 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 179.7 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 127.1 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 299.5 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 239.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 119.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 220.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 169.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 179.7 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 220.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 338.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 296.5 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 179.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 59.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 179.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 42.4 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 73.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 338.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 179.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 179.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 169.4 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 220.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 211.8 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 293.4 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 299.5 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 211.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 84.7 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 211.8 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 338.8 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 293.4 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 179.7 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 296.5 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 211.8 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 239.6 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 42.4 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 59.9 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 73.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 84.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 220.1 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 127.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 211.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 211.8 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 211.8 |
BN (mp-984) | <1 0 1> | <1 1 1> | 220.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 293.4 |
Al (mp-134) | <1 0 0> | <1 0 0> | 211.8 |
Al (mp-134) | <1 1 0> | <1 1 0> | 179.7 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 169.4 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 42.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 179.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
213 | 105 | 105 | 0 | 0 | 0 |
105 | 213 | 105 | 0 | 0 | 0 |
105 | 105 | 213 | 0 | 0 | 0 |
0 | 0 | 0 | 31 | 0 | 0 |
0 | 0 | 0 | 0 | 31 | 0 |
0 | 0 | 0 | 0 | 0 | 31 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
6.9 | -2.3 | -2.3 | 0 | 0 | 0 |
-2.3 | 6.9 | -2.3 | 0 | 0 | 0 |
-2.3 | -2.3 | 6.9 | 0 | 0 | 0 |
0 | 0 | 0 | 32.1 | 0 | 0 |
0 | 0 | 0 | 0 | 32.1 | 0 |
0 | 0 | 0 | 0 | 0 | 32.1 |
Shear Modulus GV40 GPa |
Bulk Modulus KV141 GPa |
Shear Modulus GR38 GPa |
Bulk Modulus KR141 GPa |
Shear Modulus GVRH39 GPa |
Bulk Modulus KVRH141 GPa |
Elastic Anisotropy0.38 |
Poisson's Ratio0.37 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZrInPd2 (mp-977475) | 0.0055 | 0.000 | 3 |
Ta2ReRu (mp-977357) | 0.0053 | 0.000 | 3 |
CeInAu2 (mp-636232) | 0.0051 | 0.000 | 3 |
PaInCu2 (mp-862823) | 0.0051 | 0.000 | 3 |
VGaRu2 (mp-865586) | 0.0048 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0095 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0095 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0095 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0095 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0095 | 0.000 | 4 |
GaFe3 (mp-672661) | 0.0073 | 0.036 | 2 |
Rb3Tc (mp-974820) | 0.0073 | 1.260 | 2 |
TmTe (mp-571233) | 0.0075 | 0.143 | 2 |
PmAg3 (mp-862878) | 0.0076 | 0.000 | 2 |
EuTe (mp-991027) | 0.0070 | 0.246 | 2 |
Br (mp-673171) | 0.0095 | 0.630 | 1 |
Ti (mp-73) | 0.0095 | 0.112 | 1 |
I (mp-684663) | 0.0095 | 0.446 | 1 |
Cr (mp-90) | 0.0095 | 0.000 | 1 |
Bi (mp-568610) | 0.0095 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pa Ni_pv Sn_d |
Final Energy/Atom-6.6703 eV |
Corrected Energy-26.6811 eV
-26.6811 eV = -26.6811 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)