material

Sc2IrPd

ID:

mp-862336

DOI:

10.17188/1309414


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.992 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.20 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.001 296.9
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.001 296.9
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.001 296.9
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.001 222.6
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.005 296.9
InAs (mp-20305) <1 0 0> <1 0 0> 0.009 342.8
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.015 342.8
ZnO (mp-2133) <0 0 1> <1 0 0> 0.018 299.9
SiC (mp-11714) <0 0 1> <1 1 1> 0.025 74.2
SiC (mp-7631) <0 0 1> <1 1 1> 0.030 74.2
TePb (mp-19717) <1 0 0> <1 0 0> 0.031 42.8
TePb (mp-19717) <1 1 0> <1 1 0> 0.033 60.6
BN (mp-984) <1 0 1> <1 1 1> 0.033 222.6
TePb (mp-19717) <1 1 1> <1 1 1> 0.033 74.2
MgF2 (mp-1249) <1 0 0> <1 1 0> 0.039 303.0
SiC (mp-8062) <1 0 0> <1 0 0> 0.042 171.4
SiC (mp-8062) <1 1 0> <1 1 0> 0.044 242.4
SiC (mp-8062) <1 1 1> <1 1 1> 0.044 296.9
TiO2 (mp-390) <0 0 1> <1 1 0> 0.048 303.0
SiC (mp-7631) <1 1 0> <1 1 0> 0.048 242.4
Cu (mp-30) <1 0 0> <1 0 0> 0.051 171.4
Cu (mp-30) <1 1 1> <1 1 1> 0.054 296.9
NaCl (mp-22862) <1 1 0> <1 1 0> 0.055 181.8
NaCl (mp-22862) <1 1 1> <1 1 1> 0.056 222.6
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.077 342.8
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 0 0> 0.079 214.2
Ag (mp-124) <1 0 0> <1 0 0> 0.080 85.7
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.081 42.8
Al (mp-134) <1 0 0> <1 0 0> 0.082 214.2
LaAlO3 (mp-2920) <1 0 1> <1 1 0> 0.100 303.0
LaF3 (mp-905) <1 0 0> <1 0 0> 0.104 214.2
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.105 181.8
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.113 242.4
C (mp-66) <1 1 0> <1 0 0> 0.119 342.8
TiO2 (mp-2657) <1 0 0> <1 1 1> 0.121 222.6
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.141 214.2
AlN (mp-661) <0 0 1> <1 1 0> 0.144 303.0
CdSe (mp-2691) <1 0 0> <1 0 0> 0.145 342.8
MgO (mp-1265) <1 1 1> <1 1 1> 0.152 222.6
C (mp-66) <1 0 0> <1 0 0> 0.155 214.2
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.158 214.2
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.163 342.8
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.163 299.9
AlN (mp-661) <1 1 0> <1 1 0> 0.178 242.4
Au (mp-81) <1 0 0> <1 0 0> 0.185 85.7
GaSb (mp-1156) <1 0 0> <1 0 0> 0.192 342.8
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.193 181.8
Al (mp-134) <1 1 0> <1 1 0> 0.195 181.8
YAlO3 (mp-3792) <1 0 1> <1 1 1> 0.224 148.4
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.257 60.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
177 115 115 0 0 0
115 177 115 0 0 0
115 115 177 0 0 0
0 0 0 59 0 0
0 0 0 0 59 0
0 0 0 0 0 59
Compliance Tensor Sij (10-12Pa-1)
11.6 -4.6 -4.6 0 0 0
-4.6 11.6 -4.6 0 0 0
-4.6 -4.6 11.6 0 0 0
0 0 0 16.9 0 0
0 0 0 0 16.9 0
0 0 0 0 0 16.9
Shear Modulus GV
48 GPa
Bulk Modulus KV
136 GPa
Shear Modulus GR
43 GPa
Bulk Modulus KR
136 GPa
Shear Modulus GVRH
46 GPa
Bulk Modulus KVRH
136 GPa
Elastic Anisotropy
0.52
Poisson's Ratio
0.35

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
28
U Values
--
Pseudopotentials
VASP PAW: Sc_sv Ir Pd
Final Energy/Atom
-7.6668 eV
Corrected Energy
-30.6673 eV
-30.6673 eV = -30.6673 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by