material

CdInPd2

ID:

mp-862374

DOI:

10.17188/1309435


Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.473 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.25 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.000 183.8
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.000 43.3
Ag (mp-124) <1 0 0> <1 0 0> 0.001 86.6
LiF (mp-1138) <1 0 0> <1 0 0> 0.001 216.6
C (mp-48) <0 0 1> <1 1 1> 0.001 300.1
GaSe (mp-1943) <0 0 1> <1 0 0> 0.003 303.2
CdSe (mp-2691) <1 0 0> <1 0 0> 0.004 346.5
NaCl (mp-22862) <1 1 0> <1 1 0> 0.005 183.8
NaCl (mp-22862) <1 1 1> <1 1 1> 0.006 225.1
C (mp-66) <1 0 0> <1 0 0> 0.006 216.6
SiC (mp-8062) <1 0 0> <1 0 0> 0.008 173.3
SiC (mp-7631) <1 1 0> <1 1 0> 0.009 245.0
SiC (mp-8062) <1 1 0> <1 1 0> 0.009 245.0
Au (mp-81) <1 0 0> <1 0 0> 0.012 86.6
GaSb (mp-1156) <1 0 0> <1 0 0> 0.013 346.5
Al (mp-134) <1 1 0> <1 1 0> 0.013 183.8
TePb (mp-19717) <1 0 0> <1 0 0> 0.013 43.3
TePb (mp-19717) <1 1 0> <1 1 0> 0.015 61.3
TePb (mp-19717) <1 1 1> <1 1 1> 0.015 75.0
SiC (mp-7631) <0 0 1> <1 1 1> 0.018 75.0
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.020 216.6
SiC (mp-11714) <0 0 1> <1 1 1> 0.022 75.0
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.027 346.5
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.030 61.3
PbSe (mp-2201) <1 0 0> <1 0 0> 0.032 346.5
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.035 346.5
InAs (mp-20305) <1 0 0> <1 0 0> 0.036 346.5
Si (mp-149) <1 1 1> <1 0 0> 0.045 259.9
CeO2 (mp-20194) <1 1 1> <1 0 0> 0.047 259.9
Te2Mo (mp-602) <0 0 1> <1 1 0> 0.057 306.3
TiO2 (mp-390) <0 0 1> <1 1 0> 0.058 306.3
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.060 303.2
GaN (mp-804) <1 0 0> <1 0 0> 0.061 303.2
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.067 122.5
GaN (mp-804) <0 0 1> <1 0 0> 0.067 216.6
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.069 225.1
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.069 300.1
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.070 216.6
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.070 300.1
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.070 300.1
ZnO (mp-2133) <0 0 1> <1 0 0> 0.082 303.2
BN (mp-984) <0 0 1> <1 1 0> 0.082 245.0
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.090 183.8
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.093 346.5
AlN (mp-661) <0 0 1> <1 1 0> 0.095 306.3
AlN (mp-661) <1 1 0> <1 1 0> 0.101 245.0
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.118 183.8
Te2W (mp-22693) <0 0 1> <1 1 0> 0.120 245.0
GaP (mp-2490) <1 1 1> <1 0 0> 0.121 259.9
CdTe (mp-406) <1 0 0> <1 0 0> 0.135 43.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
120 110 110 0 0 0
110 120 110 0 0 0
110 110 120 0 0 0
0 0 0 58 0 0
0 0 0 0 58 0
0 0 0 0 0 58
Compliance Tensor Sij (10-12Pa-1)
67.7 -32.4 -32.4 0 0 0
-32.4 67.7 -32.4 0 0 0
-32.4 -32.4 67.7 0 0 0
0 0 0 17.2 0 0
0 0 0 0 17.2 0
0 0 0 0 0 17.2
Shear Modulus GV
37 GPa
Bulk Modulus KV
113 GPa
Shear Modulus GR
11 GPa
Bulk Modulus KR
113 GPa
Shear Modulus GVRH
24 GPa
Bulk Modulus KVRH
113 GPa
Elastic Anisotropy
11.67
Poisson's Ratio
0.40

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiPm2Si (mp-863697) 0.0000 0.000 3
NaTl2Cd (mp-865127) 0.0000 0.000 3
TiAlPd2 (mp-865441) 0.0000 0.000 3
YbNdZn2 (mp-865843) 0.0000 0.000 3
LiHo2Tc (mp-867289) 0.0000 0.026 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.058 4
LiMgSbPt (mp-571584) 0.0000 0.051 4
LiMgSbPd (mp-10179) 0.0000 0.090 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
K3Sr (mp-973622) 0.0000 0.117 2
Yb3Re (mp-980049) 0.0000 0.551 2
ReP3 (mp-974565) 0.0000 0.826 2
Eu3Re (mp-1006150) 0.0000 0.623 2
RbBa3 (mp-975397) 0.0000 0.135 2
Br (mp-673171) 0.0000 0.630 1
Ti (mp-73) 0.0000 0.112 1
I (mp-684663) 0.0000 0.446 1
Cr (mp-90) 0.0000 0.000 1
Bi (mp-568610) 0.0000 0.139 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cd In_d Pd
Final Energy/Atom
-3.9818 eV
Corrected Energy
-15.9272 eV
Uncorrected energy = -15.9272 eV Corrected energy = -15.9272 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)