material

Sc2BeTc

ID:

mp-862563

DOI:

10.17188/1309470


Material Details

Final Magnetic Moment
0.003 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.132 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.041 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.92 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
ScBe5 + Sc + ScTc2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaAs (mp-2534) <1 0 0> <1 0 0> 0.000 165.4
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.006 165.4
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.007 286.5
Ge (mp-32) <1 0 0> <1 0 0> 0.009 165.4
C (mp-66) <1 0 0> <1 0 0> 0.011 165.4
CsI (mp-614603) <1 1 0> <1 1 0> 0.011 175.4
C (mp-66) <1 1 1> <1 1 1> 0.012 286.5
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.014 175.4
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.021 117.0
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.023 175.4
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.036 248.1
LiF (mp-1138) <1 0 0> <1 0 0> 0.040 82.7
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.048 165.4
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.054 286.5
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.063 286.5
GaN (mp-804) <0 0 1> <1 0 0> 0.071 289.5
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.071 206.8
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.072 71.6
ZnO (mp-2133) <0 0 1> <1 0 0> 0.073 330.8
KCl (mp-23193) <1 0 0> <1 0 0> 0.073 41.4
KCl (mp-23193) <1 1 0> <1 1 0> 0.078 58.5
KCl (mp-23193) <1 1 1> <1 1 1> 0.079 71.6
Mg (mp-153) <0 0 1> <1 1 0> 0.081 175.4
Ni (mp-23) <1 0 0> <1 0 0> 0.086 206.8
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.094 175.4
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.095 143.2
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.107 175.4
WS2 (mp-224) <0 0 1> <1 1 0> 0.107 175.4
Ni (mp-23) <1 1 0> <1 0 0> 0.111 330.8
Al (mp-134) <1 0 0> <1 0 0> 0.116 82.7
MgO (mp-1265) <1 0 0> <1 0 0> 0.123 165.4
SiC (mp-8062) <1 0 0> <1 0 0> 0.125 330.8
MgO (mp-1265) <1 1 0> <1 1 0> 0.131 233.9
CdS (mp-672) <1 1 1> <1 0 0> 0.132 206.8
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.151 330.8
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.153 330.8
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.161 165.4
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.162 330.8
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.169 233.9
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.170 71.6
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.191 82.7
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.206 233.9
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.211 286.5
Au (mp-81) <1 1 1> <1 1 1> 0.220 214.9
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.233 175.4
PbS (mp-21276) <1 0 0> <1 0 0> 0.233 330.8
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.238 214.9
CdS (mp-672) <0 0 1> <1 1 0> 0.239 233.9
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.259 292.4
NaCl (mp-22862) <1 0 0> <1 0 0> 0.262 165.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
146 89 89 0 0 0
89 146 89 0 0 0
89 89 146 0 0 0
0 0 0 60 0 0
0 0 0 0 60 0
0 0 0 0 0 60
Compliance Tensor Sij (10-12Pa-1)
12.6 -4.8 -4.8 0 0 0
-4.8 12.6 -4.8 0 0 0
-4.8 -4.8 12.6 0 0 0
0 0 0 16.7 0 0
0 0 0 0 16.7 0
0 0 0 0 0 16.7
Shear Modulus GV
47 GPa
Bulk Modulus KV
108 GPa
Shear Modulus GR
42 GPa
Bulk Modulus KR
108 GPa
Shear Modulus GVRH
45 GPa
Bulk Modulus KVRH
108 GPa
Elastic Anisotropy
0.68
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CeDyZn2 (mp-984702) 0.0000 0.026 3
Hf2FeTc (mp-983362) 0.0000 0.000 3
Zn2PdAu (mp-971891) 0.0000 0.008 3
Yb2TlPb (mp-864741) 0.0000 0.000 3
Tm2OsRu (mp-865383) 0.0000 0.103 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.058 4
LiMgSbPt (mp-571584) 0.0000 0.086 4
LiMgSbPd (mp-10179) 0.0000 0.074 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
K3Sc (mp-973535) 0.0000 0.615 2
Ag3Ge (mp-985283) 0.0000 0.100 2
Li3Zn (mp-976412) 0.0000 0.006 2
PmCd3 (mp-862899) 0.0000 0.000 2
Li3Pt (mp-867227) 0.0000 0.000 2
Br (mp-673171) 0.0000 0.630 1
Ti (mp-73) 0.0000 0.112 1
I (mp-684663) 0.0000 0.446 1
Cr (mp-90) 0.0000 0.000 1
Bi (mp-568610) 0.0000 0.139 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sc_sv Be_sv Tc_pv
Final Energy/Atom
-6.8236 eV
Corrected Energy
-27.2946 eV
-27.2946 eV = -27.2946 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)