material

LiCu3

ID:

mp-862658

DOI:

10.17188/1309503


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.035 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.93 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
C (mp-66) <1 0 0> <0 0 1> 0.000 12.8
LaF3 (mp-905) <1 1 0> <1 0 0> 0.003 185.4
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.003 63.9
KP(HO2)2 (mp-23959) <0 1 0> <0 0 1> 0.007 76.7
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.010 63.9
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.011 191.7
Te2Mo (mp-602) <0 0 1> <1 0 1> 0.012 88.2
KP(HO2)2 (mp-23959) <1 0 0> <0 0 1> 0.012 115.0
SrTiO3 (mp-4651) <1 1 1> <1 1 1> 0.012 277.1
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.014 63.9
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.015 197.9
WS2 (mp-224) <1 1 0> <1 0 1> 0.019 235.3
C (mp-66) <1 1 1> <1 1 1> 0.021 197.9
Ga2O3 (mp-886) <1 0 0> <1 1 1> 0.022 197.9
CaCO3 (mp-3953) <1 0 1> <0 0 1> 0.022 89.4
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.023 132.5
WS2 (mp-224) <1 1 1> <1 0 1> 0.023 235.3
TeO2 (mp-2125) <0 1 0> <1 0 1> 0.028 205.9
Ag (mp-124) <1 1 1> <1 1 0> 0.028 149.9
Ge (mp-32) <1 1 0> <1 0 1> 0.030 235.3
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.031 197.9
SiC (mp-8062) <1 1 0> <0 0 1> 0.035 191.7
GaN (mp-804) <1 0 0> <1 0 0> 0.037 185.4
AlN (mp-661) <1 0 0> <1 1 1> 0.038 79.2
LiF (mp-1138) <1 1 0> <1 0 0> 0.038 211.9
YAlO3 (mp-3792) <1 0 0> <1 0 0> 0.039 79.5
YAlO3 (mp-3792) <1 1 0> <1 1 0> 0.040 112.4
GaSe (mp-1943) <1 0 0> <0 0 1> 0.040 268.3
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.040 63.9
LiAlO2 (mp-3427) <1 1 0> <1 0 0> 0.042 185.4
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 0 1> 0.045 115.0
Au (mp-81) <1 1 1> <1 1 0> 0.046 149.9
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.047 76.7
GaAs (mp-2534) <1 1 0> <1 0 1> 0.048 235.3
Bi2Te3 (mp-34202) <0 0 1> <1 0 0> 0.048 238.4
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.049 281.1
SiC (mp-8062) <1 1 1> <1 0 1> 0.050 235.3
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.052 153.3
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.053 127.8
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.053 115.0
LaF3 (mp-905) <1 0 0> <1 0 0> 0.058 53.0
ZrO2 (mp-2858) <1 1 0> <1 0 1> 0.061 323.5
C (mp-48) <1 1 1> <1 0 1> 0.062 235.3
TiO2 (mp-2657) <1 1 0> <1 0 1> 0.066 58.8
ZnSe (mp-1190) <1 1 0> <1 0 1> 0.066 235.3
Te2Mo (mp-602) <1 0 0> <0 0 1> 0.067 166.1
NaCl (mp-22862) <1 0 0> <0 0 1> 0.071 63.9
Al2O3 (mp-1143) <1 0 0> <1 1 1> 0.071 316.7
CdS (mp-672) <0 0 1> <0 0 1> 0.072 76.7
AlN (mp-661) <1 1 1> <0 0 1> 0.073 115.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
109 83 77 0 0 0
83 109 77 0 0 0
77 77 121 0 0 0
0 0 0 61 0 0
0 0 0 0 61 0
0 0 0 0 0 59
Compliance Tensor Sij (10-12Pa-1)
24.5 -13.8 -6.8 0 0 0
-13.8 24.5 -6.8 0 0 0
-6.8 -6.8 16.9 0 0 0
0 0 0 16.3 0 0
0 0 0 0 16.3 0
0 0 0 0 0 17
Shear Modulus GV
43 GPa
Bulk Modulus KV
91 GPa
Shear Modulus GR
29 GPa
Bulk Modulus KR
90 GPa
Shear Modulus GVRH
36 GPa
Bulk Modulus KVRH
90 GPa
Elastic Anisotropy
2.49
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.0635 0.005 3
CrCoPt2 (mp-570863) 0.1555 0.034 3
LiCa6Ge (mp-12609) 0.1755 0.183 3
GaFeNi2 (mp-1065359) 0.1577 0.065 3
GaCo2Ni (mp-1018060) 0.1681 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.1835 0.028 4
CrFeCoNi (mp-1012640) 0.3138 0.065 4
CrFeCoNi (mp-1096923) 0.3616 0.193 4
Yb3U (mp-979951) 0.0099 0.633 2
Zn3C (mp-981336) 0.0168 1.046 2
Li3Be (mp-975794) 0.0160 0.242 2
Cr3Fe (mp-1017511) 0.0159 0.270 2
LiAg (mp-1018026) 0.0139 0.001 2
In (mp-85) 0.0663 0.037 1
Ce (mp-567332) 0.1442 0.000 1
Tl (mp-151) 0.1394 0.011 1
La (mp-156) 0.0677 0.001 1
Sn (mp-623511) 0.1395 0.061 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Cu_pv
Final Energy/Atom
-3.5863 eV
Corrected Energy
-14.3453 eV
Uncorrected energy = -14.3453 eV Corrected energy = -14.3453 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)