Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.606 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density14.26 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
Al (mp-134) | <1 0 0> | <1 0 0> | 0.001 | 146.7 |
Al (mp-134) | <1 1 0> | <1 1 0> | 0.001 | 207.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 0.010 | 293.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 0.011 | 146.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 0.011 | 207.5 |
C (mp-48) | <0 0 1> | <1 1 1> | 0.018 | 63.5 |
ZnO (mp-2133) | <0 0 1> | <1 1 1> | 0.022 | 254.1 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 0.039 | 155.6 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 0.042 | 293.4 |
C (mp-66) | <1 0 0> | <1 0 0> | 0.047 | 330.1 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 0.051 | 51.9 |
Ni (mp-23) | <1 1 1> | <1 1 1> | 0.051 | 63.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 0.056 | 73.3 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 0.058 | 103.7 |
Ni (mp-23) | <1 0 0> | <1 1 0> | 0.065 | 259.3 |
Au (mp-81) | <1 0 0> | <1 0 0> | 0.074 | 293.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 0.081 | 330.1 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 0.102 | 220.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 0.145 | 293.4 |
SiC (mp-11714) | <0 0 1> | <1 1 1> | 0.150 | 254.1 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 0.155 | 36.7 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 0.160 | 51.9 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 0.166 | 293.4 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 0.168 | 73.3 |
C (mp-66) | <1 1 0> | <1 1 0> | 0.184 | 311.2 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 0.186 | 190.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 0.194 | 293.4 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 0> | 0.203 | 155.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 0.223 | 293.4 |
C (mp-48) | <1 1 0> | <1 0 0> | 0.227 | 330.1 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 0.238 | 293.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 0.289 | 183.4 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 0.292 | 183.4 |
ZnO (mp-2133) | <1 0 0> | <1 1 1> | 0.303 | 317.6 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 0> | 0.303 | 155.6 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 0.325 | 36.7 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 0.328 | 146.7 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 0.336 | 51.9 |
LaF3 (mp-905) | <1 0 0> | <1 1 1> | 0.336 | 317.6 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 0.337 | 63.5 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 0.347 | 311.2 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 0.384 | 293.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 0.389 | 146.7 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 0.394 | 183.4 |
Si (mp-149) | <1 0 0> | <1 0 0> | 0.409 | 146.7 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 0.418 | 207.5 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 0.430 | 207.5 |
C (mp-48) | <1 0 1> | <1 0 0> | 0.449 | 220.0 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 0.472 | 220.0 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 0.501 | 317.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
341 | 161 | 161 | 0 | 0 | 0 |
161 | 341 | 161 | 0 | 0 | 0 |
161 | 161 | 341 | 0 | 0 | 0 |
0 | 0 | 0 | 123 | 0 | 0 |
0 | 0 | 0 | 0 | 123 | 0 |
0 | 0 | 0 | 0 | 0 | 123 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
4.2 | -1.3 | -1.3 | 0 | 0 | 0 |
-1.3 | 4.2 | -1.3 | 0 | 0 | 0 |
-1.3 | -1.3 | 4.2 | 0 | 0 | 0 |
0 | 0 | 0 | 8.1 | 0 | 0 |
0 | 0 | 0 | 0 | 8.1 | 0 |
0 | 0 | 0 | 0 | 0 | 8.1 |
Shear Modulus GV110 GPa |
Bulk Modulus KV221 GPa |
Shear Modulus GR108 GPa |
Bulk Modulus KR221 GPa |
Shear Modulus GVRH109 GPa |
Bulk Modulus KVRH221 GPa |
Elastic Anisotropy0.12 |
Poisson's Ratio0.29 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlCrRu2 (mp-862781) | 0.0000 | 0.000 | 3 |
Ti2MnNi (mp-865712) | 0.0000 | 0.000 | 3 |
TiTc2W (mp-865810) | 0.0000 | 0.000 | 3 |
Li2AcSn (mp-865913) | 0.0000 | 0.000 | 3 |
MgAlAg2 (mp-865919) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
GdF3 (mp-972965) | 0.0000 | 0.000 | 2 |
Li3Th (mp-977239) | 0.0000 | 0.416 | 2 |
In3Ga (mp-974309) | 0.0000 | 0.046 | 2 |
Ge3Sb (mp-976122) | 0.0000 | 0.334 | 2 |
V3Os (mp-866121) | 0.0000 | 0.000 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.446 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Al Zn Ir |
Final Energy/Atom-6.2766 eV |
Corrected Energy-25.1064 eV
-25.1064 eV = -25.1064 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)