Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.461 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 128.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 236.1 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 190.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 193.2 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 208.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 171.7 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 130.5 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 142.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 53.7 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 52.2 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 78.3 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 261.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 118.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 182.7 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 130.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 257.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 130.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 182.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 289.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 176.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 166.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 203.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 235.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 257.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 193.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 42.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 300.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 214.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 247.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 130.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 214.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 182.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 225.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 130.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 289.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 182.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 130.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 182.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 289.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 85.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 156.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 225.4 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 118.9 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 156.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 161.0 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 235.5 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 100.9 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 214.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 85.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 225.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
209 | 293 | 100 | 0 | 0 | 0 |
293 | 209 | 100 | 0 | 0 | 0 |
100 | 100 | 322 | 0 | 0 | 0 |
0 | 0 | 0 | 140 | 0 | 0 |
0 | 0 | 0 | 0 | 140 | 0 |
0 | 0 | 0 | 0 | 0 | 188 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-4.8 | 7.1 | -0.7 | 0 | 0 | 0 |
7.1 | -4.8 | -0.7 | 0 | 0 | 0 |
-0.7 | -0.7 | 3.5 | 0 | 0 | 0 |
0 | 0 | 0 | 7.2 | 0 | 0 |
0 | 0 | 0 | 0 | 7.2 | 0 |
0 | 0 | 0 | 0 | 0 | 5.3 |
Shear Modulus GV110 GPa |
Bulk Modulus KV191 GPa |
Shear Modulus GR1257 GPa |
Bulk Modulus KR190 GPa |
Shear Modulus GVRH684 GPa |
Bulk Modulus KVRH190 GPa |
Elastic Anisotropy-4.55 |
Poisson's Ratio-0.32 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
GaCo2Ni (mp-20551) | 0.3065 | 0.080 | 3 |
MnGaFe2 (mp-1065753) | 0.3341 | 0.037 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.5916 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.5985 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.6270 | 0.193 | 4 |
TaAl3 (mp-869) | 0.0404 | 0.000 | 2 |
Nd3Au (mp-976365) | 0.0186 | 0.207 | 2 |
Li3Tc (mp-977230) | 0.0332 | 0.624 | 2 |
Hg3Rh (mp-975452) | 0.0412 | 0.207 | 2 |
Hg3Ir (mp-981391) | 0.0330 | 0.460 | 2 |
Na (mp-974920) | 0.3641 | 0.005 | 1 |
Rb (mp-975519) | 0.2909 | 0.017 | 1 |
Ba (mp-1058581) | 0.3112 | 0.019 | 1 |
Tl (mp-151) | 0.3759 | 0.010 | 1 |
In (mp-1055994) | 0.2687 | 0.030 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Be_sv Ir |
Final Energy/Atom-5.4756 eV |
Corrected Energy-21.9024 eV
-21.9024 eV = -21.9024 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)