Final Magnetic Moment0.785 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.274 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density14.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <0 0 1> | <1 0 0> | 154.7 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 145.8 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 257.8 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 218.7 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 218.7 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 218.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 51.6 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 206.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 206.2 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 218.7 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 218.7 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 218.7 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 72.9 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 89.3 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 89.3 |
BN (mp-984) | <0 0 1> | <1 1 0> | 218.7 |
BN (mp-984) | <1 0 0> | <1 0 0> | 154.7 |
BN (mp-984) | <1 1 0> | <1 1 1> | 267.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 154.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 309.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 206.2 |
Al (mp-134) | <1 1 1> | <1 0 0> | 257.8 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 218.7 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 257.8 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 257.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 257.8 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 291.6 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 291.6 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 218.7 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 154.7 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 291.6 |
C (mp-66) | <1 0 0> | <1 0 0> | 51.6 |
C (mp-66) | <1 1 0> | <1 1 0> | 72.9 |
C (mp-66) | <1 1 1> | <1 1 1> | 89.3 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 291.6 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 218.7 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 257.8 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 309.3 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 154.7 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 154.7 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 1 0> | 218.7 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 51.6 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 145.8 |
PbS (mp-21276) | <1 1 1> | <1 0 0> | 309.3 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 257.8 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 145.8 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 309.3 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 0> | 291.6 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 257.8 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 0> | 218.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
57 | 44 | 44 | 0 | 0 | 0 |
44 | 57 | 44 | 0 | 0 | 0 |
44 | 44 | 57 | 0 | 0 | 0 |
0 | 0 | 0 | 32 | 0 | 0 |
0 | 0 | 0 | 0 | 32 | 0 |
0 | 0 | 0 | 0 | 0 | 32 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
54.2 | -23.7 | -23.7 | 0 | 0 | 0 |
-23.7 | 54.2 | -23.7 | 0 | 0 | 0 |
-23.7 | -23.7 | 54.2 | 0 | 0 | 0 |
0 | 0 | 0 | 31.1 | 0 | 0 |
0 | 0 | 0 | 0 | 31.1 | 0 |
0 | 0 | 0 | 0 | 0 | 31.1 |
Shear Modulus GV22 GPa |
Bulk Modulus KV49 GPa |
Shear Modulus GR12 GPa |
Bulk Modulus KR49 GPa |
Shear Modulus GVRH17 GPa |
Bulk Modulus KVRH49 GPa |
Elastic Anisotropy3.85 |
Poisson's Ratio0.34 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HfBe2Bi (mp-631510) | 0.0000 | 1.043 | 3 |
CaPmHg2 (mp-862883) | 0.0000 | 0.000 | 3 |
PaAlAu2 (mp-864780) | 0.0000 | 0.000 | 3 |
AcMgHg2 (mp-866225) | 0.0000 | 0.000 | 3 |
LiHo2Ir (mp-867913) | 0.0000 | 0.000 | 3 |
TiFeCoAs (mp-998974) | 0.0000 | 0.134 | 4 |
TiGaFeCo (mp-998964) | 0.0000 | 0.000 | 4 |
MnFeCoGe (mp-1018024) | 0.0000 | 0.007 | 4 |
MnGaFeCo (mp-999552) | 0.0000 | 0.044 | 4 |
AlVFeCo (mp-1008530) | 0.0000 | 0.029 | 4 |
ZrSn3 (mp-1094224) | 0.0000 | 0.444 | 2 |
Mg3Al (mp-1094666) | 0.0000 | 0.075 | 2 |
Mg3Sn (mp-1094244) | 0.0000 | 0.090 | 2 |
Sm3V (mp-972456) | 0.0000 | 0.367 | 2 |
CaMg3 (mp-1039409) | 0.0000 | 0.047 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
U (mp-108) | 0.0000 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pa Pb_d Au |
Final Energy/Atom-5.2175 eV |
Corrected Energy-20.8702 eV
-20.8702 eV = -20.8702 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)