Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.411 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 69.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 72.3 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 120.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 24.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 217.0 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 214.9 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 173.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 241.2 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 147.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 217.0 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 345.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 1> | 246.5 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 168.8 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 172.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 72.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 120.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 49.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 144.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 168.8 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 172.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 173.0 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 147.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 289.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 120.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 72.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 246.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 322.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 273.0 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 246.5 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 172.0 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 343.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 345.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 276.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 297.8 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 168.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 372.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 289.4 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 138.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 361.7 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 86.0 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 173.0 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 297.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 148.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 223.4 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 223.4 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 173.0 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 223.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 198.6 |
YVO4 (mp-19133) | <1 1 1> | <1 0 1> | 173.0 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 242.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg6SnB (mp-1099300) | 0.2510 | 0.445 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.5899 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.4931 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.5576 | 0.193 | 4 |
Pa3Nb (mp-983550) | 0.1449 | 0.176 | 2 |
SrBr3 (mp-980667) | 0.1618 | 0.321 | 2 |
NpSb3 (mp-977296) | 0.1423 | 0.194 | 2 |
HoSb3 (mp-976679) | 0.1502 | 0.172 | 2 |
Pa3Mo (mp-1006127) | 0.1349 | 0.212 | 2 |
Hg (mp-975272) | 0.4116 | 0.001 | 1 |
Cr (mp-89) | 0.3429 | 0.420 | 1 |
Tl (mp-972351) | 0.3532 | 0.000 | 1 |
Hg (mp-569360) | 0.3989 | 0.001 | 1 |
Ce (mp-20736) | 0.3728 | 0.097 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pa Ni_pv |
Final Energy/Atom-7.1244 eV |
Corrected Energy-56.9954 eV
-56.9954 eV = -56.9954 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)