Final Magnetic Moment0.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.858 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.185 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPaO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP42/mnm [136] |
Hall-P 4n 2n |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 283.7 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 160.5 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 189.9 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 189.1 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 113.9 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 197.6 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 240.7 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 170.2 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 133.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 329.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 197.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 56.7 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 283.7 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 265.8 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 32.9 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 230.5 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 56.7 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 240.7 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 265.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 302.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 151.3 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 164.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 56.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 340.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 133.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 329.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 321.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 133.7 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 56.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 208.0 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 151.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 65.9 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 113.5 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 187.2 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 214.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 65.9 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 214.0 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 132.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 56.7 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 347.7 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 98.8 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 240.7 |
BN (mp-984) | <0 0 1> | <1 1 0> | 214.0 |
BN (mp-984) | <1 0 0> | <1 0 1> | 230.5 |
BN (mp-984) | <1 0 1> | <1 0 0> | 226.9 |
BN (mp-984) | <1 1 0> | <1 0 0> | 283.7 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 215.6 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 321.5 |
Bi2Se3 (mp-541837) | <1 0 1> | <1 1 0> | 240.7 |
Al (mp-134) | <1 1 1> | <1 0 0> | 378.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
308 | 134 | 134 | 0 | 0 | 0 |
134 | 152 | 127 | 0 | 0 | 0 |
134 | 127 | 152 | 0 | 0 | 0 |
0 | 0 | 0 | 118 | 0 | 0 |
0 | 0 | 0 | 0 | 59 | 0 |
0 | 0 | 0 | 0 | 0 | 59 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
5.6 | -2.7 | -2.7 | 0 | 0 | 0 |
-2.7 | 23.2 | -17 | 0 | 0 | 0 |
-2.7 | -17 | 23.2 | 0 | 0 | 0 |
0 | 0 | 0 | 8.5 | 0 | 0 |
0 | 0 | 0 | 0 | 16.8 | 0 |
0 | 0 | 0 | 0 | 0 | 16.8 |
Shear Modulus GV62 GPa |
Bulk Modulus KV156 GPa |
Shear Modulus GR35 GPa |
Bulk Modulus KR140 GPa |
Shear Modulus GVRH49 GPa |
Bulk Modulus KVRH148 GPa |
Elastic Anisotropy3.84 |
Poisson's Ratio0.35 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SbRhO4 (mp-675025) | 0.0923 | 0.031 | 3 |
CrIrO4 (mp-769670) | 0.1777 | 0.000 | 3 |
Mo(RhO3)2 (mp-25070) | 0.2073 | 0.048 | 3 |
Hg(BiO3)2 (mp-755853) | 0.2085 | 0.013 | 3 |
CrSbO4 (mp-33857) | 0.2085 | 0.000 | 3 |
LiFe3(OF3)2 (mp-779990) | 0.3517 | 0.005 | 4 |
LiV3(OF3)2 (mp-868491) | 0.2921 | 0.000 | 4 |
LiCo3(OF3)2 (mp-850982) | 0.3110 | 0.022 | 4 |
AlSb(WO4)2 (mvc-665) | 0.3636 | 0.181 | 4 |
TiAl(WO4)2 (mvc-634) | 0.3505 | 0.100 | 4 |
IrO2 (mp-2723) | 0.0268 | 0.000 | 2 |
OsO2 (mp-996) | 0.0874 | 0.000 | 2 |
PdO2 (mp-1018886) | 0.0430 | 0.000 | 2 |
UO2 (mp-865305) | 0.0323 | 0.126 | 2 |
PtO2 (mp-1077716) | 0.0651 | 0.042 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pa O |
Final Energy/Atom-9.8601 eV |
Corrected Energy-61.9695 eV
-61.9695 eV = -59.1604 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)