Final Magnetic Moment0.017 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.336 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density13.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 119.8 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 256.8 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 183.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 169.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 89.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 329.5 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 127.1 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 209.7 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 275.3 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 110.1 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 269.6 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 146.7 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 269.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 233.0 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 329.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 42.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 239.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 89.9 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 146.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 183.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 190.6 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 105.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 190.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 169.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 89.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 84.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 110.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 329.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 360.1 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 209.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 84.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 59.9 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 211.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 89.9 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 329.5 |
Te2W (mp-22693) | <1 0 0> | <1 1 1> | 293.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 190.6 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 329.5 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 256.8 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 269.6 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 59.9 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 296.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 89.9 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 110.1 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 296.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 84.7 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 269.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 330.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 89.9 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 110.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
130 | 95 | 95 | 0 | 0 | 0 |
95 | 130 | 95 | 0 | 0 | 0 |
95 | 95 | 130 | 0 | 0 | 0 |
0 | 0 | 0 | 97 | 0 | 0 |
0 | 0 | 0 | 0 | 97 | 0 |
0 | 0 | 0 | 0 | 0 | 97 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
19.9 | -8.4 | -8.4 | 0 | 0 | 0 |
-8.4 | 19.9 | -8.4 | 0 | 0 | 0 |
-8.4 | -8.4 | 19.9 | 0 | 0 | 0 |
0 | 0 | 0 | 10.3 | 0 | 0 |
0 | 0 | 0 | 0 | 10.3 | 0 |
0 | 0 | 0 | 0 | 0 | 10.3 |
Shear Modulus GV65 GPa |
Bulk Modulus KV106 GPa |
Shear Modulus GR35 GPa |
Bulk Modulus KR106 GPa |
Shear Modulus GVRH50 GPa |
Bulk Modulus KVRH106 GPa |
Elastic Anisotropy4.41 |
Poisson's Ratio0.30 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.000 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.180 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
La3Hf (mp-973024) | 0.0000 | 0.198 | 2 |
Pr3Hf (mp-975638) | 0.0000 | 0.213 | 2 |
NiAg3 (mp-976772) | 0.0000 | 0.190 | 2 |
RuRh3 (mp-974335) | 0.0000 | 0.042 | 2 |
Tl3Hg (mp-972185) | 0.0000 | 0.020 | 2 |
P (mp-674158) | 0.0000 | 3.518 | 1 |
Xe (mp-611517) | 0.0000 | 0.006 | 1 |
Eu (mp-623532) | 0.0000 | 0.035 | 1 |
He (mp-614456) | 0.0000 | 0.008 | 1 |
Au (mp-81) | 0.0000 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pa Sb |
Final Energy/Atom-8.5042 eV |
Corrected Energy-34.2087 eV
Uncorrected energy = -34.0167 eV
Composition-based energy adjustment (-0.192 eV/atom x 1.0 atoms) = -0.1920 eV
Corrected energy = -34.2087 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)