Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.203 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 0> | 211.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 249.5 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 282.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 199.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 211.7 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 259.2 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 86.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 282.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 211.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 211.7 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 259.2 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 282.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 349.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 70.6 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 86.4 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 211.7 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 211.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 49.9 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 199.6 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 249.5 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 211.7 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 149.7 |
BN (mp-984) | <0 0 1> | <1 0 0> | 349.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 149.7 |
Al (mp-134) | <1 1 0> | <1 1 0> | 70.6 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 1> | 259.2 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 282.2 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 199.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 349.2 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 282.2 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 349.2 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 249.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 149.7 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 149.7 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 211.7 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 211.7 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 259.2 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 211.7 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 0> | 282.2 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 249.5 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 70.6 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 199.6 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 211.7 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 249.5 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 0> | 282.2 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 249.5 |
SiC (mp-11714) | <1 0 0> | <1 1 0> | 211.7 |
SiC (mp-11714) | <1 1 0> | <1 1 0> | 211.7 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 199.6 |
Au (mp-81) | <1 1 1> | <1 0 0> | 149.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
59 | 73 | 73 | -0 | -0 | 0 |
73 | 59 | 73 | -0 | -0 | 0 |
73 | 73 | 59 | -0 | -0 | 0 |
-0 | -0 | -0 | 17 | 0 | 0 |
-0 | -0 | -0 | 0 | 17 | 0 |
0 | 0 | 0 | 0 | 0 | 17 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-44.9 | 24.9 | 24.9 | 0 | 0 | 0 |
24.9 | -44.9 | 24.9 | 0 | 0 | 0 |
24.9 | 24.9 | -44.9 | 0 | 0 | 0 |
0 | 0 | 0 | 57.7 | 0 | 0 |
0 | 0 | 0 | 0 | 57.7 | 0 |
0 | 0 | 0 | 0 | 0 | 57.7 |
Shear Modulus GV8 GPa |
Bulk Modulus KV68 GPa |
Shear Modulus GR-47 GPa |
Bulk Modulus KR68 GPa |
Shear Modulus GVRH-20 GPa |
Bulk Modulus KVRH68 GPa |
Elastic Anisotropy-5.80 |
Poisson's Ratio0.66 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TmSnRh2 (mp-865252) | 0.0014 | 0.000 | 3 |
TiAlOs2 (mp-865442) | 0.0014 | 0.000 | 3 |
TmRh2Pb (mp-865787) | 0.0014 | 0.000 | 3 |
Be2CuIr (mp-867273) | 0.0016 | 0.000 | 3 |
ScMnRh2 (mp-867850) | 0.0002 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0033 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0033 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0033 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0033 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0033 | 0.000 | 4 |
MnS (mp-850100) | 0.0033 | 0.434 | 2 |
MgRe3 (mp-977283) | 0.0033 | 0.269 | 2 |
NaEr3 (mp-976405) | 0.0032 | 0.320 | 2 |
Fe9Co7 (mp-601842) | 0.0033 | 0.000 | 2 |
TiCu (mp-991438) | 0.0033 | 0.083 | 2 |
Br (mp-673171) | 0.0033 | 0.630 | 1 |
Ti (mp-73) | 0.0033 | 0.112 | 1 |
I (mp-684663) | 0.0033 | 0.446 | 1 |
Cr (mp-90) | 0.0033 | 0.000 | 1 |
Bi (mp-568610) | 0.0033 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pm_3 Ag |
Final Energy/Atom-3.5153 eV |
Corrected Energy-14.0614 eV
-14.0614 eV = -14.0614 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)