Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.371 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.091 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 254.0 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 167.6 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 215.5 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 119.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 215.5 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 191.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 152.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 263.4 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 205.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 33.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 47.9 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 169.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 152.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 215.5 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 205.3 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 117.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 203.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 270.9 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 88.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 304.8 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 205.3 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 263.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 287.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 287.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 215.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 84.7 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 88.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 95.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 135.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 215.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 47.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 167.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 191.6 |
BN (mp-984) | <0 0 1> | <1 1 1> | 88.0 |
BN (mp-984) | <1 0 0> | <1 0 0> | 287.8 |
BN (mp-984) | <1 0 1> | <1 1 0> | 191.6 |
BN (mp-984) | <1 1 0> | <1 1 1> | 263.9 |
BN (mp-984) | <1 1 1> | <1 1 0> | 239.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 152.4 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 215.5 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 205.3 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 205.3 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 254.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 33.9 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 47.9 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 169.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 16.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 23.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 118.5 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 1 0> | 119.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr8Ni50Mo15W2 (mp-767372) | 0.4343 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.5955 | 0.057 | 4 |
MgPa3 (mp-976742) | 0.0000 | 0.190 | 2 |
Ce3Br (mp-984727) | 0.0000 | 0.403 | 2 |
EuPd3 (mp-636279) | 0.0000 | 0.032 | 2 |
EuNi3 (mp-974834) | 0.0000 | 0.306 | 2 |
Sm3Ho (mp-978949) | 0.0000 | 0.017 | 2 |
LiCa6Ge (mp-12609) | 0.0000 | 0.184 | 3 |
ZnCu2Ni (mp-30593) | 0.4436 | 0.002 | 3 |
Cr22Ni50Mo3 (mp-767825) | 0.4406 | 0.000 | 3 |
GaCo2Ni (mp-1018060) | 0.1699 | 0.080 | 3 |
CrCoPt2 (mp-570863) | 0.2277 | 0.035 | 3 |
He (mp-614456) | 0.0000 | 0.009 | 1 |
Xe (mp-611517) | 0.0000 | 0.005 | 1 |
Eu (mp-623532) | 0.0000 | 0.075 | 1 |
P (mp-674158) | 0.0000 | 3.510 | 1 |
S (mp-684673) | 0.0000 | 1.298 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points108 |
U Values-- |
PseudopotentialsVASP PAW: Pm_3 Rh_pv |
Final Energy/Atom-7.0694 eV |
Corrected Energy-28.2775 eV
-28.2775 eV = -28.2775 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)